Unless otherwise agreed, the steel surface temperature generally should be at least 3°C (5°F) above the dew point temperature when paints are used. If the PosiTector DPM senses a smaller difference (delta value), three things happen: the contrast of the display reverses, the red LED emits, and the meter’s alarm beeps.