| Specifications |
Range |
Accuracy |
Resolution |
Surface
Temperature |
–40° to 80° C |
±0.5° C |
0.1° C |
| 80° to 190° C |
±1.5° C |
| –40° to 175° F |
±1° F |
0.1° F |
| 175° to 375° F |
±3° F |
Air
Temperature |
–40° to 80° C |
±0.5° C |
0.1° C |
| –40° to 175° F |
±1° F |
0.1° F |
| Humidity |
0 to 100% |
±3% |
0.1% |
Conforms to: ISO
8502-4 , BS
7079-B4, ASTM
D3276-05 , and SSPC-PA7
 |
PosiTector DPM comes complete with...
- humidity, air and surface temperature sensors
- protective rubber holster with belt clip and wrist strap
- 3 AAA batteries
- instructions
- nylon carrying case with shoulder
strap
- Certificate of Calibration traceable to NIST
- two (2)
year warranty (Body and
Sensors)
|
|
| Instrument Dimensions |
7" x
2.5" x 1.2"
178 x 64 x 31 mm |
| Weight (without batteries) |
185 g (6.5 oz.) |
|