  PosiTest®  Pull-Off Adhesion Tester
Measures adhesion of coatings to metal, wood, concrete and other substrates
PosiTest AT - Overview  PosiTest AT - Two Models  PosiTest AT - Rugged Features  PosiTest AT - Technical Data  PosiTest AT - Optional Accessories  PosiTest AT - Q&A  PosiTestAT - Download Literature  Application Assistance Request Form

 

Technical Data (AT-M manual and AT-A automatic)

Conforms to national and international standards including ASTM D4541/D7234,
ISO 4624/16276-1, AS/NZS 1580.408.5 and others

Resolution: 1 psi (0.01 MPa)

Accuracy: ± 1% Full Scale

Adhesion
Strength

Dolly Size
Max Pull-Off Pressure
10 mm
10000 psi
70 MPa
14 mm
6000 psi
40 MPa
20 mm*
3000 psi
20 MPa
50 mm**
500 psi
3.5 MPa
   *supplied with PosiTest AT    **requires 50mm kit

Warranty: 2 Years

   
 Both Kits include:  
  • Adhesion tester with digital display
  • 20 mm aluminum test dollies (20)
  • Abrasive pad
  • Cutting tool
  • Adhesive with mixing sticks and palettes
  • Cotton swabs
  • Instruction booklet
  • Certificate of Calibration traceable to NIST
  • Instructional Video
  • Sturdy, lightweight carrying case
  • Two-year warranty
  • Built-in rechargeable NiMH batteries with recharger/AC power supply.
  • Shoulder strap (AT-A only)

Weight of Kit (with case) :
12 lbs / 5.5 kg

Carrying Case Dimensions:
L – 17 in / 43 cm
W – 13 in / 33 cm
H – 6 in / 15 cm


Aluminum Test Dollies