PosiTector Inspection Kit (KITFNS1) contains a Standard(1) PosiTector body, PosiTector 6000 separate ferrous/non-ferrous coating thickness probe, PosiTector SPG surface profile probe, and a PosiTector DPM environmental probe.

Each PosiTector body accepts the 6000, DPM, and SPG probes included in the kit easily converting from a coating thickness gage to a dew point meter or surface profile gage.

Build your own custom kit - add additional probes such as the PosiTector 200 (ultrasonic coating thickness), UTG (ultrasonic wall thickness) or RTR (replica tape reader).

 

  Standard and Advanced Kits - Feature Comparison Selected

Order Code

KITFNS1 KITFNS3
 

  PosiTector body features

Standard (1) Advanced (3)

Accepts all PosiTector 6000, 200, DPM, UTG, SPG and RTR probes. View Video 

High Contrast LCD Display

Color Color
USB port for fast, simple connection to a PC and to supply continuous power. USB cable included
PosiSoft USB – stored readings and graphs can be accessed using universal PC/Mac web browsers or file explorers. No software required
Connects to PosiSoft.net - free web-based application offering secure storage of thickness readings
Software updates via web keep your gage current

WiFi technology wirelessly synchronizes with PosiSoft.net, downloads software updates, and connects to mobile devices for expanded functionality

 

Bluetooth Wireless Technology for data transfer to a PC or optional portable printer View Video 

 

Real Time Graphing, Picture Prompting, Batch Notes and Onscreen help

 
  PosiTector SPG Surface Profile Probe specific features Standard (1) Advanced (3)

All features shown on PosiTector SPG overview page

Statistics - Instantly calculate average, standard deviation, min/max thickness and number of readings while measuring

Hi-Lo limits audibly and visibly alerts when measurements exceed your specified limits

Reading Storage Capacity

250 in
one group
100,000 in up to
1000 groups

SmartBatch™ allows entry of user-defined parameters and criteria to comply with various standards and test methods

 
  PosiTector DPM Environmental probe specific features Standard (1) Advanced (3)

All features shown on PosiTector DPM overview page

Dataset Storage Capacity (1 dataset = RH, Ta, Ts, Td, Ts–Td) Stored readings can be viewed or downloaded

2,500 in
one group
20,000 in up to
1000 groups

Auto Log Mode automatically records all 5 parameters at user selected time intervals. Runs unattended on batteries or continuously via USB. View Video 

Unattended battery life (using 3 AAA alkaline batteries)

up to 50 hours up to 8 months

Stream datasets via USB or Bluetooth wireless at specified Auto Log intervals. Ideal for remote monitoring.

 

Trend Charts graph readings in real-time View Video 

 

User defined limits for all parameters with visible and audible warnings

 
  PosiTector 6000 Coating Thickness probe specific features Standard (1) Advanced (3)

All features shown on PosiTector 6000 overview page

Statistics - Instantly calculate average, standard deviation, min/max thickness and number of readings while measuring

FAST mode  faster measurement speed for quick inspection

SCAN mode  take continuous readings without lifting the probe

 

Hi-Lo Limits  audibly and visibly alerts when measurements exceed your specified limits

Reading Storage Capacity

250 in
one group
100,000 in up to
1000 groups

SSPC PA2 feature set determines if film thickness over a large area conforms to user-specified min/max levels

 

PSPC 90/10 feature determines if a coating system complies with an IMO performance standard for protective coatings

 

Multiple stored calibration adjustments for measuring on a variety of substrate conditions

 

 

KITFNS1 comes complete with a Standard(1) gage body, separate ferrous/non-ferrous coating thickness probe (6000-FNS), environmental probe, surface profile probe, precision plastic shims, glass zero plate and metal shim, protective rubber holster with belt clip, wrist strap, 3 AAA alkaline batteries, 3 instruction manuals, hard shell case, protective lens shield, 3 Long Form Certificates of Calibration traceable to NIST or PTB, USB cable and 2 year warranty on gage body and probes.

Case Size: 30 cm (l) x 25 cm (w) x 10 cm (d),    12” (l) x 10” (w) x 4” (d)

Weight: 1.3 kg (2.8 lbs.)

 



[