The PosiTector 200 measures coating thickness over wood, concrete, plastics, composites, metals and more using ultrasonic technology. It consists of a body (Standard or Advanced) and probe (200 B, C or D).

 

Step 1: Select a Body (Standard or Advanced features)


Includes ALL features as shown on Overview page plus...

  • Hi Contrast reversible color LCD
  • Storage of 250 readings in one group – stored readings can be viewed or downloaded

 

 

 

Includes ALL features as shown on Overview page plus...

  • Measure the total thickness of a coating system or up to 3 individual layer thicknesses in a multi-layer system. Also features graphic readout for detailed analysis of the coating system.
  • Graphics mode with screen capture
  • Hi Contrast reversible color LCD
  • Storage of 100,000 readings in up to 1,000 batches and sub-batches
  • Store thickness, profile, environmental and wall thickness measurements in individual batches
  • Onscreen Batch Annotation -add notes, change batch names, and more with the new built‐in QWERTY keyboard
  • WiFi technology wirelessly synchronizes with PosiSoft.net, downloads software updates, and connects to mobile devices for expanded functionality
  • PosiSoft Mobile - gage-based software application allows access to readings, graphs, capture photos and update notations through WiFi enabled devices such as tablets, smart phones and computers
  • Bluetooth Wireless Technology for data transfer to a computer or optional portable printer
    View Video
     
  • Onscreen help, Real time graphing, picture prompting, and more . . .

PosiTector Body Comparison Chart

 

Step 2: Select a Probe (200 B, 200 C or 200 D) 


 

PosiTector 200 Probes B C D
 
 Probe Model (Order Code) PRB200B PRB200C PRB200D
 Typical Applications polymer coating on
wood, plastic, etc.
Coatings on concrete,
fiberglass, etc.
Thick, soft coatings like
polyurea, asphaltic neoprene,
very thick polymers
 Measurement Range* 13 to 1000 μm
0.5 to 40 mils
50 to 3800 μm
2 to 150 mils
50 to 7600 μm
2 to 300 mils
 Accuracy + (2 μm + 3% of reading)
+ (0.1 mils + 3% of reading)
+ (20 μm + 3% of reading)
+ (1 mils + 3% of reading)

Advanced Models: Minimum Individual Layer Thickness**

13 μm
0.5 mils
50 μm
2 mils
500 μm
20 mils

*Range limits apply to polymer based coatings only. D probe polyurea range is 50 to 5000 μm (2 to 200 mils)
**For multiple layer applications only. Dependent on material to be tested

 



[