PosiTector® 200 Series
Coating Thickness Gages for wood, concrete, plastic and more...
PosiTector 200 - Overview PosiTector 200 - Rugged Features PosiTector 200 - Gage Selection PosiTector 200 - Probe Details PosiTector 200 - Ordering Chart PosiTector 200 - Optional Accessories PosiTector 200 - Download Literature Application Assistance Request Form
Probe Details: Two probe configurations are available for measuring a wide variety of coating thickness application.
PosiTector 200
Probe Model:
B C
Range*

13 - 1000 um
0.5 -40 mils

50 - 3800 um
2 - 150 mils
Typical Applications:
Polymer coatings on
wood, plastic,
composites, etc.
Thicker coatings
on concrete,
fiberglass, etc.
Accuracy:
± (2 microns + 3% of reading)
± (0.1 mils + 3% of reading)
*Range limits apply to polymer coatings only.