| Created: | 2011-04-18 00:06:51 |
| Gage S/N: | 702272 |
| Probe Type: | F |
| Probe S/N: | 157953 |
| CAL: | Cal 1 |
| Units: | microns |
![]() | ![]() | ![]() | ![]() | ![]() |
|---|---|---|---|---|
| 10 | 18.4 | 2.8 | 15 | 25 |
![]() | ||
|---|---|---|
| 1 | 25 microns | 2011-04-18 00:06:56 |
| 2 | 16 microns | 00:06:58 |
| 3 | 19 microns | 00:07:00 |
| 4 | 18 microns | 00:07:02 |
| 5 | 16 microns | 00:07:04 |
| 6 | 19 microns | 00:07:06 |
| 7 | 18 microns | 00:07:08 |
| 8 | 15 microns | 00:07:09 |
| 9 | 19 microns | 00:07:11 |
| 10 | 19 microns | 00:07:13 |