The Measure of Quality
 

PosiTector® 6000 Series
Coating Thickness Gage for ALL Metal Substrates
>> PosiTector 6000 - Features

 

Rugged Features (Advanced model shown in Memory Mode)



 

 

360° Viewer (Advanced model shown in Real Time Graphing Mode)


Due to security settings of some browsers (like preventing accessing of local file config.xml from within a webpage), please upload the content of the output folder to an online location to experience full functionality. This message will hide automatically when online.

 

 

 


Memory & USB Mass Storage


The PosiTector 6000 can record coating thickness measurements for on-screen statistical purposes, for printing to an optional Bluetooth wireless printer (Advanced models only), for transferring to a computer or synchronizing with PosiTector.net. Readings are time-stamped as they are taken.

Memory Capacity

Standard models:  250 readings in one group
Advanced models: 100,000 measurements in up to 1000 groups (batches)

USB Mass Storage

The PosiTector 6000 uses a USB mass storage device class which provides a simple interface to retrieve data in a manner similar to USB flash drives, cameras, or digital audio players.

 

 

Any computer can view and download measurements stored in memory (in batches) by navigating a virtual drive labeled PosiTector using the included USB cable.


A formatted HTML report is viewed by selecting the “index.html” file found in the root directory. Additionally, delimited text files (.txt) are located in each batch folder for easy import into database, spreadsheet and other compatible applications.

Sample HTML formatted report