The Measure of Quality
Since 1966
Products
Contact Us
Service & Support
Application Notes
Technical Notes
Technology Center
International Standards
Downloads
What's New
 
Espanol Deutsch Français 中文 English

PosiTector® 6000 Series
Coating Thickness Gages for ALL metal substrates
PosiTector 6000 - Overview PosiTector 6000 - Rugged Features PosiTector 6000 - Gage Selection PosiTector 6000 - Probe Details PosiTector 6000 - Ordering Chart PosiTector 6000 - Optional Accessories PosiTector 6000 - Download Literature Application Assistance Request Form
Probe Details: Several probe configurations are available for measuring a wide variety of coating thickness application.


Selection Note:

F - for ferrous metals (i.e. FS)
N - for non-ferrous metals (i.e. PosiTector 6000 NS)
FN - for all metal substrates (i.e. PosiTector 6000 FNS)

 Built-in probes

Built-in Probe
Gage Models:
F1, F2, F3
N1, N2, N3
FN1, FN2, FN3
FT1, FT2, FT3
Range:
0 - 60 mils 0 -250 mils
0 - 1500 um 0 - 6 mm
Accuracy*:
+ (0.05 mils + 1%)  0 - 2 mils
   + (0.1 mils  +  1%)  > 2 mils
+ (0.5 mils + 1%)  0 - 100 mils
 + (0.5 mil + 3%) > 100 mils
+ (1 um + 1%)  0 - 50 um
 + (2 um + 1%)  > 50 um

 + (0.01 mm + 1%) 0 - 2.5 mm
+ (0.01 mm + 3%) > 2.5 mm

*Accuracies are stated as a fixed value plus a percentage of the gage's actual reading.

 

 Separate Regular Probes (below regular probes suitable for underwater use)

Regular
Probe Models:
FS
NS
FNS
NAS
FTS
Range:
0 - 60 mils 0 -25 mils 0 -250 mils
0 - 1500 um 0 - 625 um 0 - 6 mm
Accuracy*:
+ (0.05 mils + 1%)  0 - 2 mils
   + (0.1 mils  +  1%)  > 2 mils
+ (0.02 mils + 1%)  0 - 4 mils
 + (0.1 mils + 3%)  > 4 mils
+ (0.5 mils + 1%)  0 - 100 mils
 + (0.5 mil + 3%) > 100 mils
+ (1 um + 1%)  0 - 50 um
 + (2 um + 1%)  > 50 um
+ (.5 um + 1%)  0 - 100 um
 + (2 um + 3%)  > 100 um
 

 + (0.01 mm + 1%) 0 - 2.5 mm
+ (0.01 mm + 3%) > 2.5 mm

*Accuracies are stated as a fixed value plus a percentage of the gage's actual reading.

 

90 Regular
Probe Models:
FRS
NRS
FNRS
Range:
0 - 60 mils
0 - 1500 um
Accuracy*:
+ (0.05 mils + 1%)  0 - 2 mils
   + (0.1 mils  +  1%)  > 2 mils
+ (1 um + 1%)  0 - 50 um
 + (2 um + 1%)  > 50 um
*Accuracies are stated as a fixed value plus a percentage of the gage's actual reading.

 Separate Microprobes

0 Microprobe
Probe Models:
F0S
N0S
Range:
0 - 45 mils 0 - 25 mils
0 - 1150 um 0 - 625 um
Accuracy*:
+ (0.02 mils + 1%)  0 - 4 mils
 + (0.1 mils + 3%)  > 4 mils
+ (.5 um + 1%)  0 - 100 um
 + (2 um + 3%)  > 100 um
  
*Accuracies are stated as a fixed value plus a percentage of the gage's actual reading.

 

45 Microprobe
Probe Models:
F45S
N45S
Range:
0 - 45 mils 0 - 25 mils
0 - 1150 um 0 - 625 um
Accuracy*:
+ (0.02 mils + 1%)  0 - 4 mils
 + (0.1 mils + 3%)  > 4 mils
+ (.5 um + 1%)  0 - 100 um
 + (2 um + 3%)  > 100 um
  
*Accuracies are stated as a fixed value plus a percentage of the gage's actual reading.

 

90 Microprobe
Probe Models:
F90S
N90S
Range:
0 - 45 mils 0 - 25 mils
0 - 1150 um 0 - 625 um
Accuracy*:
+ (0.02 mils + 1%)  0 - 4 mils
 + (0.1 mils + 3%)  > 4 mils
+ (.5 um + 1%)  0 - 100 um
 + (2 um + 3%)  > 100 um
  
*Accuracies are stated as a fixed value plus a percentage of the gage's actual reading.

 Separate High-Range Probes

High-Range
Probe Models:
FNTS
FKS
NKS
Range:
0 -250 mils 0 -500 mils
0 - 6 mm 0 - 13 mm
Accuracy*:
+ (0.5 mils + 1%)  0 - 100 mils
 + (0.5 mil + 3%) > 100 mils
+ (1 mils + 3%)  0 - 500 mils
 + (0.02 mm + 3%) 0 - 13 mm

 + (0.01 mm + 1%) 0 - 2.5 mm
+ (0.01 mm + 3%) > 2.5 mm