PosiPen®Magnetic
pull-off thickness gage
measures non-magnetic coatings such as paint,
enamel, |
PosiPen
is manufactured in three versions:
- PosiPen Model A for measurements on surfaces with normal temperatures
- PosiPen Model B for measurements on surfaces with extreme temperatures (between -150°F and +450°F or -100°C and +230°C)
- PosiPen Model C ferrite comparator
PosiPen A and B have two scales, microns (metric) and mils (inch)
![]() |
Range: 0.25 to 20 mils
(inch) Tolerance ±10% and 0.1 mil Range: 5 to 500 microns (metric) Tolerance ±10% and 2.5 microns |
PosiPen A and B are calibrated to NIST calibration standards.