The Measure of Quality
 

 

DeFelsko Products Applicable Standards

Magnetic Coating Thickness (ferrous substrates)

ISO 2064

“Metallic and other inorganic coatings -- Definitions and conventions concerning the measurement of thickness”

ISO 1461

“Hot dip galvanized coatings on fabricated iron and steel articles -- Specifications and test methods”

ISO 2808

“Paints and Varnishes - Determination of Film Thickness”

ISO 2178

“Non-Magnetic Coatings on Magnetic Substrates – Measurement of Coating Thickness - Magnetic Method”

ISO 2361

Electrodeposited nickel coatings on magnetic and non-magnetic substrates -- Measurement of coating thickness -- Magnetic method

ISO 19840

“Paints and varnishes -- Corrosion protection of steel structures by protective paint systems -- Measurement of, and acceptance criteria for, the thickness of dry films on rough surfaces”

Eddy Current Coating Thickness (non-ferrous substrates)

ISO 2360

“Non-Conductive Coatings on Non-Magnetic Basis Metals – Measurement of Coating Thickness - Eddy Current Method"

PosiTector 200 Ultrasonic Coating Thickness (non-metal substrates)

ISO 2808

“Paints and Varnishes - Determination of Film Thickness"

PosiTector DPM - Dew Point Meter

ISO 8502-4

“Preparation of steel substrates before application of paints and related products -- Tests for the assessment of surface cleanliness -- Part 4: Guidance on the estimation of the probability of condensation prior to paint application”

PosiTest AT - Pull-Off Adhesion Tester

ISO 4624

“Paints and Varnishes – Pull-off Test for Adhesion”

ISO 16276-1

"Corrosion protection of steel structures by protective paint systems -- Assessment of, and acceptance criteria for, the adhesion/cohesion (fracture strength) of a coating -- Part 1: Pull-off testing"