The Measure of Quality
Product News

 



   

 

  PosiTector RTR H1 H3 P1 P3
 

 Order Code

RTR H1 RTR H3 RTR P1 RTR P3
 Included PosiTector Body Standard Advanced Standard Advanced
 Included PosiTector Probe PRBRTRH PRBRTRP
 Measure Peak Height (HL) All models
 Measure Peak Density (Pd)    
 Generate 2D/3D images       with Advanced body
 Save SDF Surface Data Files       with Advanced body

 Peak Height (HL)
 
Measurement Range

20 to 115 μm (0.8 to 4.5 mils)
 Peak Height (HL) Accuracy + 5 μm (+ 0.2 mils)
 Peak Height (HL) Resolution + 1 μm (+ 0.2 mils)
 Anvil Diameter Ø6.3 mm (Ø0.25 inch)
 Anvil Pressure

110 gram-force (1.1 Newtons)

 

ALL GAGES COME COMPLETE with stainless steel burnishing tool, 5 cleaning cards, check shim(s), surface cleaning putty, protective rubber holster with belt clip, wrist strap, 3 AAA alkaline batteries, instructions, nylon carrying case with shoulder strap, protective lens shield, Long Form Certificate of Calibration traceable to PTB, USB cable, two year warranty on body and probe.

Replica Tape not included

SIZE: 152 x 61 x 28 (6” x 2.4” x 1.1”)
WEIGHT: 140 g (4.9 oz.) without batteries

CONFORMS TO: ASTM D4417, NACE RP0287, SSPC PA 17, SSPC-SP5, SP6, SP10, SP11-87T,
AS 3894.5, ISO 8503-5 and others

 



[
What's New]