Non-Certified Plastic Shim Specifications


 

Microns Mils Accuracy (±) Color Couleur Farbe Color
25 1 20% Orange Orange Orange Naranja
50 2 10% Red Rouge Rot Rojo
125 5 5% Blue Bleu Blau Azul
250 10 5% Brown Brun Braun Marron
505 20 5% Yellow Jaune Gelb Amarillo