Pre-programmed Material Velocities
Material (Menu
Option) |
Longitudinal
Velocity |
Min
Range* |
Max
Range* |
| in/us |
m/s |
in |
mm |
in |
mm |
| CAST
IRON (Iron) |
0.179 |
4547 |
0.040 |
1.02 |
5.000 |
127.00 |
| SS
303 (SS303) |
0.223 |
5664 |
0.040 |
1.02 |
5.000 |
127.00 |
| STEEL
1018 (Steel) |
0.233 |
5918 |
0.040 |
1.02 |
5.000 |
127.00 |
| Al
2024 (Alum) |
0.251 |
6375 |
0.050 |
1.27 |
5.000 |
127.00 |
| PLEXIGLAS
(Plexi) |
0.106 |
2692 |
0.040 |
1.02 |
2.000 |
50.80 |
| PVC
(PVC) |
0.094 |
2388 |
0.035 |
0.89 |
2.000 |
50.80 |
| POLYSTYRENE
(Poly) |
0.081 |
2057 |
0.035 |
0.89 |
2.000 |
50.80 |
* Range may change depending on surface roughness,
Temperature or Material Properties. |