PosiTector UTG Ultrasonic Thickness Gages
   
A variety of accessories are available to help you get the most from your PosiTector UTG.

Certified Step Blocks

Ideal for checking calibration and operation of ultrasonic thickness gages and are an important component in fulfilling both ISO and in-house quality control requirements.

  • Composition - 1018 steel
    - available in metric and imperial units
    - metric units: (2.5, 5, 7.5, 10 and 12.5 mm steps)
    - imperial units: (100, 200, 300, 400 and 500 mil steps)
    - metric accuracy ±0.02 mm
    - imperial accuracy ±1 mil
  • All Certified Step Blocks are supplied with a certificate of calibration showing traceability to NIST/NPL.

 

Ultrasonic Couplant

Every PosiTector UTG ships with (1) bottle of Ultrasonic couplant.  Additional 4oz. bottles are available.
(sold in cases of 12). MSDS 

Bluetooth Printer receives data from Advanced models

  • Receives data via Bluetooth wireless technology.
  • Prints readings and statistical summary
  • Battery-operated
  • Light weight
  • One year Warranty

Bluetooth Transfer Overview 


PosiTector Probes

PosiTector body accepts all PosiTector 6000, 200, DPM, UTG, RTR and SPGprobes easily converting from a coating thickness gage to a dew point meter, surface profile gage or wall thickness gage

 

 

AC Power Cable for continuous operation or battery charging

This kit supplies several alternate power solutions for your battery-operated PosiTector. They allow the gage to operate continuously without the need for batteries.

Use the cable alone to connect a PosiTector to your PC's built-in USB port that acts as a continuous power source. Or connect the cable to the included power adaptor which plugs into any AC wall electrical outlet, 110 or 220V.

A selection of electrical plugs is included which are capable of dealing with most country’s outlets.

 

PosiTector Case

Convenient hard shell case for carrying a PosiTector gage body and multiple probes - including any of the PosiTector 6000 Coating Thickness probes, DPM Dew Point Meter probes, SPG Surface Profile probes, or UTG Ultrasonic Wall Thickness probes.

Case has compartments for Certificates of Calibration, instruction manuals and other accessories. 

Rechargeable Batteries

  • eneloop HR4UTG (NiMH 800 AAA 1.2V)
  • Precharged and ready to use immediately
  • Considerably longer run time than conventional Nickel Cadmium batteries
  • Low self-discharge: once charged, eneloop rechargeable batteries keep 90% of their charge after 6 months and 85% after 12 months
  • High performance at low temperatures down to -10 °C
  • No charger required - Recharge batteries inside the PosiTector when connected via USB.
  • eneloop website: http://www.eneloop.info

 

Protective Lens Shield

  • Pack of five thin plastic lens shields
  • Ideal for protecting the PosiTector display from paint overspray.

One lens shield is included with every PosiTector instrument

 



[
What's New]
[Products ] [Service & Support] [Join our Team]
[Terms & Conditions] [Privacy] [Resources] [Contact Us]
[Site Map]

©2017 DeFelsko Corporation.