 PosiTector UTG Corrosion Multiple Echo


 Order Code

UTG C1 UTG C3 UTG M1 UTG M3
 Included Body Standard Advanced Standard Advanced
 Included Probe UTG C UTG M
 Probe Type 5 MHz Dual Element 5 MHz Contact
 Thru-Paint Capability (Multiple Echo) no yes
 Measurement Range* - Single Echo 0.040" to 5.000"
1.00 to 125.00 mm
0.100" to 5.000"
2.50 to 125.00 mm
 Measurement Range* - Multiple Echo NA 0.100" to 2.500"
2.50 to 60.00 mm
 Resolution 0.001"
0.01 mm
0.001"
0.01 mm
 Accuracy ±0.001"
±0.03 mm
±0.001"
±0.03 mm
* Measurement range is for carbon steel and depends upon surface condition, temperature and material.

 

ALL GAGES COME COMPLETE with body and probe, couplant, protective rubber holster with belt clip, wrist strap, 3 AAA alkaline batteries, instructions, nylon carrying case with shoulder strap, protective lens shield, Long Form Certificate of Calibration traceable to NIST, USB cable, PosiTector.net account, two (2) year warranty.

SIZE: 146 x 61 x 28 (5.75” x 2.4” x 1.1”)

WEIGHT: 140 g (4.9 oz.) without batteries

CONFORMS TO: ASTM E797

 

 



[