The Measure of Quality
Product News

 



PosiTector UTG

THEORY OF OPERATION

PosiTector UTG probes transmit an ultrasonic pulse into the material to be measured. This pulse travels through the material towards the other side. When it encounters an interface such as air (back wall) or another material, the pulse is reflected back to the probe. The time required for the pulse to propogate through the material is measured by the gage, represented as t1 and t2 below.

Single Echo

PosiTector UTG C probes feature a dual element transducer with automatic V-Path compensation. Thickness is determined by measuring t1 (uncoated) or t2 (coated), dividing it by two and then multiplying by the velocity of sound for that material (steel). See Figure 1.

 

  Figure 1 t2 > t1

For uncoated materials t1 relates directly to material thickness. When a material is coated the propagation time is increased and is shown above as t2.

Coatings such as paint have a slower velocity of sound than that of metal. Thus the single echo technique will produce a thickness result greater than the actual combined coating+metal thickness. The result will include a significantly higher, unknown value of paint thickness. Therefore it is not a simple matter of measuring the thickness of the paint and subtracting it from the single echo measurement result.

 

Multiple Echo

PosiTector UTG M probes determines thickness by measuring the time between at least three consecutive back wall echoes.

 

  Figure 2 t1 = t2 = t3

In Figure 2 above, multiple echo mode measures only the time between echoes. Regardless of whether the steel is coated or not, all times between echoes are the same. In multiple-echo mode the gage determines thickness by measuring t1+ t2+ t3, dividing it by six and then multiplying by the velocity of sound for that material. The resultant thickness calculation made by the instrument is therefore an accurate measurement of the steel thickness only, disregarding the coating thickness.

The velocity of sound is expressed in inches per microsecond or meters per second. It is different for all materials. For example, sound travels through steel faster (~0.233 in/µs) than it travels through plastic (~0.086 in/µs).

 

 


[