Step 1. Place the tip of the PosiPen on the coated surface and allow the magnet to contact.

Step 2. Pull the PosiPen straight back from the object to be measured while keeping close watch on the appropriate indicator.

Note the reading when the magnet releases.

 



Hover over image for demonstration
 

   

 

 

Triple Indicator: compensates for gravity

The PosiPen compensates for gravity when measuring in different positions.

1. Use the red/silver joining line when the Gage is horizontal (walls).
2. Use the green line when the Gage is pointing straight down (green/ground).
3. Use the blue line when the Gage is pointing straight up (blue/sky).

 

 

 