uparrow-iconp0chonk

PosiTest®

Magnetic Coating Thickness Gages for Non-Magnetic Coatings on Steel

PosiTest magnetic pull-off thickness gage (banana gauge) for the non-destructive measurement of non-magnetic coatings (paint, enamel, galvanizing, metalizing, plating, etc.) on steel.

  • Highly wear resistant Carbide Probe for longest life and continuous accuracy
  • Extra rugged housing, not affected by mechanical shock, water, acid or solvents
  • Unique overall design, fully supported, positive positioning, no pivoting tendencies during measurement
  • Positive visual and audible indicators to designate when thickness reading is established
  • “V” grooves in probe housing and gage base allow correct positioning on cylindrical objects
  • Certificate of Calibration showing traceability to PTB included (Long Form)
Conforms to ASTM D7091/B499, ISO 2808 and others

Features

Accurate

  • Certificate of Calibration showing traceability to PTB included with every gage
  • Matching Calibration Standards and Procedures available for every model
  • Highly wear resistant Carbide Probe for longest life and continuous accuracy
  • Remove center of dial cover for easy calibration adjustment
  • Conforms to national and international standards

Durable

  • Extra rugged housing, not affected by mechanical shock, water, acid or solvents
  • Unique overall design, fully supported, positive positioning, no pivoting tendencies during measurement
  • Can be used fully supported or with only the front probe area contacting the surface
  • Functions on a permanent rare-earth cobalt magnet
  • No batteries/electronics
  • 2 year warranty
The PosiTest easily measures small parts of almost any shape
Easily measures small parts of almost any shape

Simple

  • Positive visual and audible indicators to designate when thickness reading is established
  • “V” grooves in probe housing and Gage base allow correct positioning on cylindrical objects
  • Compact, lightweight, precisely balanced, independent of gravity – can be used in any position
  • GO/NO-GO button can be pre-set for rapid measurement
  • Probe contact and dial rotation all in a one-finger operation
  • Furnished with wrist strap and instructions in a high quality leather case with belt loops for your convenience
carbide measuring probe for long life
Carbide measuring probe for long life

Models

Choose from four models:

illustration of PosiTest FM scale
PosiTest FM
Application
Hot dip galvanizing, hard chrome metalizing, paint, enamel, plastic coatings on steel.
Scale FM
0-80 mils
Tolerance:
± 0.2 mils up to 4 mils
±5% of the reading over 4 mils
View PDFAdd to Instant Quote
illustration of PosiTest F scale
PosiTest F
Application
Hot dip galvanizing, hard chrome metalizing, paint, enamel, plastic coatings on steel.
Scale F
0-2000 µm
Tolerance:
±5 µm up to 100 µm
±5% of the reading over 100 µm
View PDFAdd to Instant Quote
illustration of PosiTest GM scale
PosiTest GM
Application
Electroplating,
thin paint films, 
phosphating on steel.
Scale gM
0-8 mils
Tolerance:
±0.04 mils up to 0.8 mils
±5% of the reading over 0.8 mils
View PDFAdd to Instant Quote
illustration of PosiTest G scale
PosiTest G
Application
Electroplating,
thin paint films, 
phosphating on steel.
Scale g
0-200 µm
Tolerance:
±1 µm up to 20 µm
±5% of the reading over 20 µm
View PDFAdd to Instant Quote

Videos

Video Thumbnail
PosiTest - Magnetic Pull-off Thickness Gage
Video Thumbnail
DeFelsko Coating Thickness Gages | 2023

F.A.Q.

plus-icon
minus-icon

Is the PosiTest calibrated at the factory?

The PosiTest arrives fully calibrated and ready to measure. A Long-Form Certificate of Calibration traceable to NIST or PTB is included, which documents actual readings taken by your instrument at our calibration laboratory on standards traceable to a national metrology institute. Beware of ‘Certificates’ or ‘Certificates of Conformance’ offered by competitors. These typically do not include actual instrument readings, and are often insufficient to meet common quality requirements. The PosiTest features a rare-earth permanent magnet that prevents any kind of drift over time. A PosiTest gage that sits unused on a shelf for several years will not drift or lose its calibration.

plus-icon
minus-icon

Is the PosiTest intrinsically safe?

“Intrinsically Safe” (I.S.) is commonly used to describe electronic products destined for a hazardous (explosive) operating environment. Owing to the mechanical (non-electronic) design of the PosiTest, it does not require certification as an “intrinsically safe” device.

plus-icon
minus-icon

Why should I purchase the PosiTest over the PosiPen?

Compared with the PosiPen, the PosiTest provides superior accuracy and improved ease-of-use by using a large dial to increase spring pressure, and by holding the displayed gage reading after being removed from the coated part. The PosiPen is ideal for small, hot or hard-to-reach surfaces.

plus-icon
minus-icon

Is the PosiTest affected by the roughness of the steel substrate below the coating?

All coating thickness gages are influenced to some degree by substrate roughness. It is generally accepted that coating thickness should be measured from the highest ‘peaks’ in the rough surface thus ensuring they are covered by the protective coating. However, coating thickness gages will instead measure the coating thickness from the effective magnetic surface, which is located somewhere between the highest peaks and deepest valleys of the profile.

To compensate for the influence of substrate conditions (including roughness), measure the uncoated substrate/part at a number of spots to obtain a representative average value. This average value is called the “base metal reading” or “BMR”. Subtract the BMR from subsequent coating thickness measurements to obtain the thickness of the coating over the ‘peaks’ of the rough surface.

plus-icon
minus-icon

Can the PosiTest measure nickel on steel?

Yes, but it depends upon the particular type of nickel coating that has been applied to the steel.

When nickel plating is deposited by a process of electrolysis (employing an electric current in the nickel bath), the resultant coating – commonly called “e-nickel” – is always conductive and magnetic to some degree and cannot be accurately measured by our gages when applied to ferrous or non-ferrous metals.

Electroless nickel coatings are deposited by an autocatalytic process which does not involve the addition of an electric current. If the nickel bath in this process contains a minimum concentration of ~8% phosphorus, the resulting nickel plating is effectively non-magnetic and its thickness can be accurately measured on ferrous steel with a magnetic principle coating thickness gage such as the PosiTest.

plus-icon
minus-icon

Does the PosiTest measure on hot surfaces?

The operating temperature range of the PosiTest depends on the use case. The first case is where the measurement surface and the gage are both at the same temperature;  in this case the operating range would be -10°C to 60°C (14°F to 140°F). The other case is where the PosiTest is at a “normal” room temperature but the measurement sample may be at a different temperature. In this case the PosiTest can measure on surfaces with temperatures ranging from -50°C to 100°C (-58°F to 212°F), so long as the instrument itself is kept within its operating range.

plus-icon
minus-icon

Can the PosiTest be used underwater?

Yes. The PosiTest features corrosion-resistant brass construction and can be immersed in fresh or saltwater. When used in saltwater, it is recommended to rinse with freshwater after use.

plus-icon
minus-icon

Can the PosiTest be adjusted?

While the PosiTest can be adjusted, this is not recommended for most applications. The permanent rare-earth magnet eliminates the need for adjustment, unlike other mechanical instruments. If a PosiTest is not functioning properly in accordance with NIST / PTB calibration standards we recommend the Gage be returned to us for a no-cost evaluation. Opening the PosiTest for purposes of cleaning, re-balancing and recalibration is not recommended.

plus-icon
minus-icon

Does the PosiTest measure on non-ferrous metals, like aluminum?

No. As a magnetic principle instrument, the PosiTest will measure the thickness of non-magnetic coatings applied to ferrous metals. Our popular PosiTest DFT Combo and powerful PosiTector 6000 N gage models are ideal for measuring the thickness of paint, anodize and other non-conductive coatings applied to non-ferrous metals.

plus-icon
minus-icon

Is the PosiTest ‘automatic’?

The PosiTest is a simple, manually-operated coating thickness gage. The GO/NO-GO button can be preset for taking rapid, accurate measurements.

Resources

Downloads

Information