The Measure of Quality
 

Certified & Non-Certified Plastic Shims

For use with magnetic, eddy-current and ultrasonic coating thickness gages.
(Not intended for use with Type 1 magnetic pull-off type gages)

 
   
Shims Overview  
  • Simulate a coating over a particular substrate material or shape. Gage performance can be conveniently verified on a regular basis as required by some international test methods
  • For use with all Type 2, electronic coating thickness gages
  • Protects the probe from damage or premature wear when placed over hot or abrasive surfaces
  • Can be placed on top of soft or tacky coating films to obtain thickness measurements without the gage probe depressing the coating film

Certified Plastic Shims

  • Certified shims provide an economical alternative to Coated Metal Plates but have a reduced accuracy
  • Certified Plastic Shims are available in the following thicknesses (all thicknesses are approximate):
Order
Code
Approximate
Thickness
Color
Accuracy
CS1
25 µm (1 mil)
Orange ±2 µm (±0.08 mil)
CS2
50 µm (2 mil)
Red
CS3
75 µm (3 mil)
Green
CS5
125 µm (5 mil)
Blue
CS10
250 µm (10 mil)
Brown
CS20
500 µm (20 mil)
Yellow
CS40
1000 µm (40 mil)
White
CS60
1500 µm (60 mil)
Black
CSS
Complete set of 8
  • Each shim is packaged in their own plastic protective pouch
  • Certificate of Calibration showing traceability to NIST is included with each shim or set of shims
  • Certified and labeled in both Metric and Imperial units

 

 

Non-Certified Plastic Shims

  • Provide a quick operational check of the instrument by allowing the user to perform practice measurements
  • Can be used to protect the probe when measuring on tacky, rough or hot surfaces
  • Labeled in both Metric and Imperial units
  • Available as a set of 5 (below)
Approximate
Thickness
Color
Accuracy
25 µm (1 mil)
Orange ± 20%
50 µm (2 mil)
Red ± 10%
125 µm (5 mil)
Blue ± 5%
250 µm (10 mil)
Brown ± 5%
500 µm (20 mil)
Yellow ± 5%

A package of 5 non-certified shims is included with all DeFelsko electronic coating thickness gages (Type 2).