PosiTector® RTR H

Electronic Surface Profile Gage for Blasted Steel and Textured Coatings

Digital Micrometer for measuring Testex® Press-O-Film® replica tape—compatible with the PosiTector gage body.

  • Ready to measure—no calibration adjustment required for most applications
  • Large 2.8" impact resistant color touchscreen with redesigned keypad for quick menu navigation
  • Weatherproof, dustproof, and water-resistant—IP65-rated enclosure
  • PosiTector interchangeable platform—attach any PosiTector probe to a single gage body
  • USB, WiFi, and Bluetooth connectivity to PosiSoft PC, Mac, and Smartphone software
  • Certificate of Calibration showing traceability to PTB included (Long Form)
Conforms to ASTM D4417, ISO 8503-5, NACE SP0287, SSPC-PA 17, SSPC-SP5, SP6, SP10, SP11-87T, and others

Features

simple icon

Simple

  • Measures surface profile height using replica tape in accordance with ASTM D4417, ISO 8503-4, and NACE SP0287
  • Large 2.8" impact resistant color touchscreen with redesigned keypad for quick menu navigation
  • On-gage help explains menu items at the touch of a button
  • RESET feature instantly restores factory settings
durable icon

Durable

  • Weatherproof, dustproof, and water-resistant—IP65-rated enclosure
  • Rugged indoor/outdoor instrument—ideal for field or shop use
  • Ergonomic design with durable rubberized grip
  • Shock-absorbing, protective rubber holster for added impact resistance
  • Two year warranty on gage body AND probe
accurate icon

Accurate

  • Simply select the appropriate replica tape grade to automatically apply the appropriate conversion factor and subtract the 50 µm (2 mils) backing thickness
  • Certificate of Calibration showing traceability to PTB included (Long Form)
  • Conforms to national and international standards including ISO 8503-5, ASTM D4417 Method C, NACE RP0287 and SSPC-PA17
versatile icon

Versatile

  • PosiTector body accepts all PosiTector 6000, 200, RTR, SPG, DPM, IRT, SST, UTG, SHD, BHI, and GLS probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, ultrasonic wall thickness gage, hardness tester, or gloss meter
  • Mils/Microns switchable
  • Selectable display languages
  • Auto rotating display with Flip Lock

Standard Models

Includes ALL features as shown on left plus...
Includes ALL features as shown above plus...
  • Storage of 1,000 readings per probe—stored readings can be viewed or downloaded

Advanced Models

Includes ALL features as shown on left plus...
Includes ALL features as shown above plus...
  • Storage of 250,000 readings from multiple probes in up to 1,000 batches
  • Live graphing of measurement data
  • Touchscreen keyboard for quickly renaming batches, adding notes, and more
  • WiFi technology wirelessly synchronizes with PosiSoft.net and downloads software updates
  • Bluetooth 4.0 Technology for data transfer to a mobile device running the PosiTector App or optional portable printer. BLE API available for integration into third-party software.
  • Integrate with third-party software, drones, ROVs, PLCs, and robotic devices using several industry-standard communication protocols
powerful icon

Powerful

  • Statistics mode continually displays/updates average, standard deviation, min/max, and number of readings while measuring
  • Screen Capture—save 100 screen images for record keeping and review
  • Instant-on feature quickly powers up the gage if recently powered down
  • Over 20 hours of continuous operation with 3 AAA batteries
  • USB port for fast, simple connection to a PC and to supply continuous power. USB cable included
  • PosiSoft USB Drive—stored readings and graphs can be accessed using universal PC/Mac web browsers or file explorers. No software required.
  • Every stored measurement is date and time stamped
  • Software Solutions for viewing, analyzing & reporting data
  • Software Updates via web keep your gage current

Specifications

20 to 115 μm
(0.8 to 4.5 mils)
Peak Height (HL) Accuracy
± 5 μm (± 0.2 mils)
Peak Height (HL) Resolution
1 μm (0.1 mils)
Anvil Diameter
Ø6.35 mm (Ø0.25 inch)
Anvil Pressure
1.1 Newtons (110 gram-force)
Size*
127 x 66 x 25.4 mm
(5" x 2.6" x 1")
Weight*
Peak Height (HL)
Measurement Range
137 g (4.9 oz.) without batteries

* Size and weight are for the PosiTector gage body only and do not include the probe.

View More Features

How It Works

prepare the surface with cleaning putty

1

Prepare

Use cleaning putty to remove dust, debris, or residual blast media from the measurement site by firmly pressing the putty onto the surface to be tested using your fingers and remove.

burnish the replica tape

2

Burnish

Select the appropriate grade of replica tape, then pull a single piece of tape free of its release paper and apply to blasted surface.

Firmly compress replica film using burnishing tool by applying sufficient pressure in a circular and x-y rubbing motion. When complete, remove tape from surface.

Photo—closeup of the anvils of the PosiTector RTR measuring Replica Tape

3

Measure

Insert the compressed replica tape between the micrometer's measurement anvils and take a reading.

Ensure the tape is properly positioned so that the burnished region is centered in the anvils with the adhesive side down.

illustration showing how replica tape works

Models

Step 1: Choose a gage body

Step 2: Select A Model

Click model to download cutsheet
PosiTector RTR with standard gage body
RTR H1
Peak Height (HL) Measurement Range
20 to 115 μm (0.8 to 4.5 mils)
Peak Height (HL) Accuracy
± 5 μm (± 0.2 mils)
Peak Height (HL) Resolution
1 μm (0.1 mils)
Anvil Diameter
Ø6.3 mm (Ø0.25 inch)
Anvil Pressure
1.1 Newtons (110 gram-force)
View PDFView PDFAdd to Instant Quote

Step 2: Select A Model

Click model to download cutsheet
PosiTector RTR with advanced gage body
RTR H3
Peak Height (HL) Measurement Range
20 to 115 μm (0.8 to 4.5 mils)
Peak Height (HL) Accuracy
± 5 μm (± 0.2 mils)
Peak Height (HL) Resolution
1 μm (0.1 mils)
Anvil Diameter
Ø6.3 mm (Ø0.25 inch)
Anvil Pressure
1.1 Newtons (110 gram-force)
View PDFView PDFAdd to Instant Quote

Step 2: Select A Model

Click model to download cutsheet
PosiTector RTR probe
PRBRTRH
Peak Height (HL) Measurement Range
20 to 115 μm (0.8 to 4.5 mils)
Peak Height (HL) Accuracy
± 5 μm (± 0.2 mils)
Peak Height (HL) Resolution
1 μm (0.1 mils)
Anvil Diameter
Ø6.3 mm (Ø0.25 inch)
Anvil Pressure
1.1 Newtons (110 gram-force)
View PDFView PDFAdd to Instant Quote
SmartLink and app in use

PosiTector SmartLink - A Smart New Way to Measure

PosiTector SmartLink and free mobile app turns your cell phone or tablet into a virtual PosiTector gage.

Wirelessly connect PosiTector probes to your Apple iOS or Android smart device.

For more information about the PosiTector SmartLink, click here.

Videos

Video Thumbnail
How to Measure Surface Profile using Testex Replica Tape and the PosiTector RTR
Video Thumbnail
Saving Money and Time with PosiTector Probe Interchangeability
Video Thumbnail
New PosiTector Gage Body
Video Thumbnail
PosiTector SmartLink

Software

PosiSoft Software in use

PosiSoft Desktop

Powerful desktop software for downloading, archiving, and reporting measurement data. No internet connection required.

  • Simple, intuitive user interface
  • Import readings directly from the gage via USB, WiFi, or legacy PosiSoft Desktop versions
  • Fully integrates with PosiSoft.net—backup and synchronize jobs, batches, readings, and report templates to the cloud. Click here to learn more about PosiSoft.net
Learn More

PosiTector App

An easy-to-use mobile app (iOS/ Android) that connects to your PosiTector Advanced, PosiTector Smartlink, or PosiTest AT-A. Compatible with PosiSoft.net.

Learn More

PosiSoft USB

A simple gage interface to retrieve data in a manner similar to a flash drive. No software to install or internet connection required.

Learn More

PosiSoft Custom PDF Report Generator

featured on PosiSoft Desktop, PosiSoft.net, PosiTector App
Easily create reports from your measurement data in seconds
  • Generate custom, professional PDF reports
  • Include inspection information such as on-site pictures, screen captures, notes and more to communicate important details
  • Create and save multiple custom layouts as templates – insert cover pages, add logos/images, and select font and point size
  • Select the information to include for each product type – charts, histograms, readings, time stamps and more
  • Compile multi-batch reports from one or more probes and instrument types

PosiSoft.net

PosiSoft.net is a free cloud-based application offering secure storage of PosiTector and PosiTest Inspection Instrument data. Click Here to learn more.

PosiTector Developer Resources

From wired USB to WiFi wireless technology, DeFelsko instruments offer data management solutions for even the most advanced software integrations. Accessing your stored or live streaming data is simpler and more flexible than ever before. PosiTector and PosiTest AT-A instruments have the ability to integrate with third-party software, drones, ROVs, PLCs, and robotic devices using several industry-standard communication protocols.

Learn More about Integrating Third-Party Devices and Applications

F.A.Q.

plus-icon
minus-icon

Is the PosiTector RTR H calibrated at the factory?

The PosiTector RTR arrives fully calibrated and ready to measure. A Long-Form Certificate of Calibration traceable to NIST is included, which documents actual readings taken by your instrument at our calibration laboratory on standards traceable to a national metrology institute. Beware of ‘Certificates’ or ‘Certificates of Conformance’ offered by competitors. These typically do not include actual instrument readings, and are often insufficient to meet common quality requirements.

Verification of gage calibration and accuracy can be performed with the supplied check shim, which is specifically intended for all PosiTector RTR probes. 

plus-icon
minus-icon

What is replica tape?

Replica tape is a long-known method for characterizing a surface. It is simple, relatively inexpensive, and shows good correlation with results from other methods. It has the advantages of ruggedness, relatively low start-up cost, good repeatability and the option of retaining a physical replica of the surface being evaluated. The method is widely used and widely understood. It is particularly useful for measurements on curved surfaces that are difficult to measure directly with other instruments.

It is therefore not surprising that it has become the most popular field method for measuring surface profile. Its operation is described in a number of international standards including ASTM D4417, ISO 8503-5, NACE SP0287, and AS 3894.5.

plus-icon
minus-icon

What grades of replica tape is the PosiTector RTR H compatible with?

The PosiTector RTR H is compatible with the four primary grades of replica tape: Coarse Minus, Coarse, X‐Coarse, and X-Coarse Plus. The PosiTector RTR H automatically corrects for the non-linearity of Coarse, X-Coarse, and X-Coarse Plus tape.

Note: Coarse Minus replica tape does not require conversion.

plus-icon
minus-icon

Is the PosiTector RTR H as accurate as conventional spring micrometers?

Yes. Unlike some conventional spring micrometers, the PosiTector RTR  series and Testex Digital Micrometer feature a Conversion Mode (HL) which adjusts for the non-linearity of replica tape displaying a more accurate surface profile measurement.

plus-icon
minus-icon

How many readings are required for each location?

At least two measurements should be taken at each location. If the two replicas differ by 5 µm (0.2 mils) or less, their average should be recorded as the profile.

If the two initial replicas differ by more than 5 µm (0.2 mils), a third replica is recommended. The average of the two closest replicas should be recorded.

plus-icon
minus-icon

Why does the blasted steel under the burnished replica tape appear shiny, and different from the surrounding area?

Abrasive blasting often leaves debris on the surface, which changes its appearance. If the surface isn’t cleaned with the included cleaning putty before measuring, the replica tape captures this debris and ‘cleans’ the surface where the tape was burnished. This may make the test area appear ‘shiny’ compared to the surrounding area, and is not a sign of damage to the blast profile.

plus-icon
minus-icon

Should I purchase the PosiTector RTR Replica Tape Reader or PosiTector SPG Surface Profile Gage for my application?

Both instruments conform to ASTM D4417 "Standard Test Methods for Field Measurement of Surface Profile of Blast Cleaned Steel".

The PosiTector SPG conforms to Method B of ASTM D4417. The PosiTector SPG measures quickly, and has no per-test cost. It keeps a digital record of each measurement, is less operator dependent, as no burnishing of replica tape is required. It also has a greater range than replica tape.

The PosiTector RTR conforms to Method C of ASTM D4417. It is used together with Testex Replica Tape, a widely used and respected method to measure surface profile. It has the ability to measure on curved surfaces, and gives the user the option to retain the replica tape; a physical replica of the tested surface.

plus-icon
minus-icon

What is the spring pressure on the probe? Do I have to apply a specific pressure to the buttons?

The anvil impact force of the PosiTector RTR is identical to that of conventional mechanical spring micrometers. The PosiTector RTR has the same anvil size (0.25 inch / 6.25mm diameter) and applies the same spring tension (110 gram‐force / 1.1 Newtons) as Testex micrometers and as required by major test standards.

An issue with mechanical spring micrometers is that they can under‐read if a user drops the measuring anvils onto the replica tape too fast. Other errors can occur if the user presses upward on measuring arms to “stabilize” readings. Both actions force conventional micrometers to read lower by crushing the tape’s delicate microfoam.

The PosiTector RTR’s unique opposing spring design prevents these undesired user interferences from occurring. Pressing the two probe buttons releases a holding spring. That allows a second spring, the anvil spring, to apply a constant pressure measuring force on the replica. This measuring force is not coupled to the buttons so the user cannot alter the applied pressure and inadvertently influence results.

plus-icon
minus-icon

How often should the PosiTector probe be recalibrated?

PosiTector probes include a Certificate of Calibration showing traceability to NIST or PTB included (Long Form) with each probe—with no expiry or end date. They have no shelf life, therefore the length of time in the field is not a good indicator for recalibration intervals. Many organizations with quality programs and recertification programs require annual recalibrations, and this is a good starting point for most users. DeFelsko recommends that customers establish calibration intervals based upon their own experience and work environment. Based on our product knowledge, data and customer feedback, a one year calibration interval from the date the instrument was placed in service is a good starting point.

plus-icon
minus-icon

Do your instruments require any formal training for use? Do you offer ‘demo’ models?

No. The PosiTector RTR Replica Tape Reader is designed for simple operation, featuring easy-to-use menus, an instruction manual, and helpful videos. In lieu of demonstration models, we provide unlimited technical support via telephone and/or email, and a limited 30-day money back guarantee.

plus-icon
minus-icon

Still need help?

Before returning your gage or instrument for service, review the troubleshooting steps on the Troubleshooting guide, or speak with a member of our technical support team by calling +1-315-393-4450.

Accessories

PosiTector Gage BodiesPosiTector Gage Bodies

PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.

Learn MoreLearn More
PosiTector ProbesPosiTector Probes

PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.

Learn MoreLearn More
Bluetooth PrinterBluetooth Printer

Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.

Learn MoreLearn More
PosiTector CasePosiTector Case

Convenient hard shell case for carrying a PosiTector gage body and multiple probes

Learn MoreLearn More
Testex™ Press-O-Film™ Replica TapeTestex™ Press-O-Film™ Replica Tape

Each roll of Testex Tape includes 50 pieces (Impressions)

Learn MoreLearn More
Testex Certified Shim SetTestex Certified Shim Set

Used to verify the accuracy and operation of all Testex micrometers. Ideal for fulfilling both ISO and in-house quality control requirements. Includes Certificate of Calibration traceable to PTB.

‍

Learn MoreLearn More
AC Power KitAC Power Kit

Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.

Learn MoreLearn More
Pelican Cases for PosiTector Inspection KitsPelican Cases for PosiTector Inspection Kits

Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTector instrument.

Learn MoreLearn More
PosiTector RTR Check ShimPosiTector RTR Check Shim

Used to check PosiTector RTR peak height accuracy (RTR H and RTR 3D). One check shim is included with each probe.

Learn MoreLearn More
Surface Cleaning PuttySurface Cleaning Putty

To clean the test surface of debris prior to burnishing

Learn MoreLearn More
Cleaning CardsCleaning Cards

Pre-moistened with isopropyl alcohol to clean residual adhesive and debris from the PosiTector RTR and RTR 3D anvils helping to ensure an accurate test.

Learn MoreLearn More
High Accuracy Burnishing ToolHigh Accuracy Burnishing Tool

Burnishing tool includes a built-in spring mechanism ensuring that consistent force is used, regardless of how hard the tool is pressed against the surface

Learn MoreLearn More
Belt ClipBelt Clip

Belt Clip for PosiTector gage bodies

Learn MoreLearn More
Protective Lens ShieldProtective Lens Shield

Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.

Learn MoreLearn More
View More Accessories

Resources

Downloads

Information