uparrow-iconp0chonk

PosiTector® 200

Coating Thickness Gages for Non-Metal Substrates

Non-destructively measures a wide variety of applications using proven ultrasound technology. Measure coating thickness over wood, concrete, plastic, and more. Advanced models measure up to 3 layers with graphics.

  • Ready to measure—no calibration adjustment required for most applications
  • Large 2.8" impact resistant color touchscreen with redesigned keypad for quick menu navigation
  • Weatherproof, dustproof, and water-resistant—IP65-rated enclosure
  • PosiTector interchangeable platform—attach any PosiTector probe to a single gage body
  • USB, WiFi, and Bluetooth connectivity to PosiSoft PC, Mac, and Smartphone software
  • Certificate of Calibration showing traceability to NIST or PTB included (Long Form)
Conforms to ASTM D6132 and ISO 2808/193397

Features

simple icon

Simple

  • Ready to measure—no adjustment required for most applications
  • Large 2.8" impact resistant color touchscreen with redesigned keypad for quick menu navigation
  • On-gage help explains menu items at the touch of a button
  • RESET feature instantly restores factory settings
durable icon

Durable

  • Weatherproof, dustproof, and water resistant—IP65-rated enclosure
  • Ergonomic design with durable rubberized grip
  • Shock-absorbing, protective rubber holster for added impact resistance
  • Two year warranty on gage body AND probe
accurate icon

Accurate

  • Responsive transducers provide fast, accurate readings
  • Certificate of Calibration showing traceability to NIST or PTB included
  • Proven non-destructive ultrasonic technique conforms to ASTM D6132 and ISO 2808
versatile icon

Versatile

  • PosiTector body accepts all PosiTector 6000, 200, RTR, SPG, DPM, IRT, SST, UTG, SHD, BHI, and GLS probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, ultrasonic wall thickness gage, hardness tester, or gloss meter
  • Auto rotating display with Flip Lock
  • Mils/Microns switchable
  • Selectable display languages
powerful icon

Powerful

  • Continually displays/updates average, standard deviation, min/max, and number of readings while measuring
  • Max Thick Mode displays the deepest ultrasonic echo eliminating the need to adjust the Lo Range—ideal for ignoring unwanted surface echoes
  • Screen Capture – save 100 screen images for record keeping and review
  • Over 20 hours of continuous operation with 3 AAA batteries
  • USB port for fast, simple connection to a PC and to supply continuous power. USB cable included.
  • PosiSoft USB Drive—stored readings and graphs can be accessed using universal PC/Mac web browsers or file explorers. No software required.
  • Includes PosiSoft suite of software for viewing and reporting data
  • Software Updates via web keep your gage current

Standard Models

Includes ALL features as shown on left plus...
Includes ALL features as shown above plus...
  • Measure the total thickness of a coating system
  • Storage of 1,000 readings per probe—stored readings can be viewed or downloaded

Advanced Models

Includes ALL features as shown on left plus...
Includes ALL features as shown above plus...
  • Measure the total thickness of a coating system or up to 3 individual layer thicknesses in a multi-layer system.
  • Graphics mode with screen capture for detailed analysis of the coating system
  • Storage of 250,000 readings in up to 1,000 batches
  • Prompted Batch Mode—create pre-defined batches with on-screen text and image prompts for each reading
  • Live graphing of measurement data
  • SSPC-PA 9 modes help users comply with standards by prompting for min/max specifications, displaying the necessary readings, and automatically calculating statistics with a pass/fail result
  • Touchscreen keyboard for quickly renaming batches, adding notes, and more
  • Multiple stored calibration adjustments for measuring on a variety of coating applications
  • WiFi technology wirelessly synchronizes with PosiSoft.net and downloads software updates
  • Bluetooth 4.0 Technology for data transfer to a mobile device running the PosiTector App or optional portable printer. BLE API available for integration into third-party software.
  • Integrate with third-party software, drones, ROVs, PLCs, and robotic devices using several industry-standard communication protocols
View More Features

Models

externallink-icon
View PDF Order Guide

Step 1: Choose a gage body

Step 2: Select a Model

Click model to download cutsheet
All PosiTector 200 models measure total thickness
PosiTector 200 B1 probe
200 B1
Application
Polymer coating on wood, plastic, etc.
Measurement Range*
13 to 1,000 μm
0.5 to 40 mils
Accuracy
± (2 μm + 3% of reading)
± (0.1 mils + 3% of reading)
Certified Thickness Standard
STDA3
View PDFAdd to Instant Quote
PosiTector 200 C1 probe
200 C1
Application
Coatings on concrete, fiberglass, etc.
measurement Range*
50 to 3,800 μm
2 to 150 mils
Accuracy
± (2 μm + 3% of reading)
± (0.1 mils + 3% of reading)
CERTIFIED THICKNESS STANDARD
STDP6
View PDFAdd to Instant Quote
PosiTector 200 D1 probe
200 D1
Application
Thick, soft coatings like polyurea, asphaltic neoprene, very thick polymers
measurement Range*
50 to 7,600 μm     2 to 300 mils
Accuracy
± (20 μm + 3% of reading)
± (1 mil + 3% of reading)
CERTIFIED THICKNESS STANDARD
STDP1
View PDFAdd to Instant Quote
*Range limits apply to polymer based coatings only. D probe polyurea range is 50 to 5,000 μm (2 to 200 mils).

Step 2: Select a Model

Click model to download cutsheet
All PosiTector 200 Advanced models measure individual layers
PosiTector 200 B3 probe
200 B3
Application
Polymer coating on wood, plastic, etc.
Measurement Range*
13 to 1,000 μm
0.5 to 40 mils
Accuracy
± (2 μm + 3% of reading)
± (0.1 mils + 3% of reading)
MINIMUM INDIVIDUAL LAYER THICKNESS**
13 μm
0.5 mils
Certified Thickness Standard
STDA3
View PDFAdd to Instant Quote
PosiTector 200 C3 probe
200 C3
Application
Coatings on concrete, fiberglass, etc.
Measurement Range*
50 to 3,800 μm
2 to 150 mils
Accuracy
± (2 μm + 3% of reading)
± (0.1 mils + 3% of reading)
Minimum Individual layer thickness**
50 μm
2 mils
CERTIFIED THICKNESS STANDARD
STDP6
View PDFAdd to Instant Quote
PosiTector 200 D3 probe
200 D3
Application
Thick, soft coatings like polyurea, asphaltic neoprene, very thick polymers
Measurement Range*
50 to 7,600 μm     2 to 300 mils
Accuracy
± (20 μm + 3% of reading)
± (1 mil + 3% of reading)
Minimum Individual layer thickness**
500 μm
20 mils
CERTIFIED THICKNESS STANDARD
STDP1
View PDFAdd to Instant Quote
*Range limits apply to polymer based coatings only. D probe polyurea range is 50 to 5,000 μm (2 to 200 mils).
**For multiple layer applications only. Dependent on material to be tested.

Step 2: Select a Model

Click model to download cutsheet
PosiTector PRB200B probe
PRB200B
Application
Polymer coating on wood, plastic, etc.
Measurement Range*
13 to 1,000 μm
0.5 to 40 mils
Accuracy
± (2 μm + 3% of reading)
± (0.1 mils + 3% of reading)
Certified Thickness Standard
STDA3
View PDFAdd to Instant Quote
PosiTector PRB200C probe
PRB200C
Application
Coatings on concrete, fiberglass, etc.
Measurement Range*
50 to 3,800 μm
2 to 150 mils
Accuracy
± (2 μm + 3% of reading)
± (0.1 mils + 3% of reading)
CERTIFIED THICKNESS STANDARD
STDP6
View PDFAdd to Instant Quote
PosiTector PRB200D probe
PRB200D
Application
Thick, soft coatings like polyurea, asphaltic neoprene, very thick polymers
Measurement Range*
50 to 7,600 μm     2 to 300 mils
Accuracy
± (20 μm + 3% of reading)
± (1 mil + 3% of reading)
CERTIFIED THICKNESS STANDARD
STDP1
View PDFAdd to Instant Quote
*Range limits apply to polymer based coatings only. D probe polyurea range is 50 to 5,000 μm (2 to 200 mils).

Videos

Video Thumbnail
How to Measure Thickness of Rough Coatings using PosiTector 200 Ultrasonic Coating Thickness Gage
Video Thumbnail
PosiTector 200 Medición de espesor en superficies rugosas
Video Thumbnail
DeFelsko Coating Thickness Gages | 2023
Video Thumbnail
How to Use the PosiTector 200 to Measure Paint/Coating on Wood, Plastic, Concrete, and More
Video Thumbnail
Saving Money and Time with PosiTector Probe Interchangeability
Video Thumbnail
How To Use Prompted Batch Mode to Simplify Inspections and Maximize Performance
Video Thumbnail
New PosiTector Gage Body
Video Thumbnail
PosiTector 200 - Coating Thickness Measurement on Rough Surfaces

Software

PosiSoft Software in use

PosiSoft Desktop

Powerful desktop software for downloading, archiving, and reporting measurement data. No internet connection required.

  • Simple, intuitive user interface
  • Import readings directly from the gage via USB, WiFi, or legacy PosiSoft Desktop versions
  • Fully integrates with PosiSoft.net—backup and synchronize jobs, batches, readings, and report templates to the cloud. Click here to learn more about PosiSoft.net
Learn More

PosiTector App

An easy-to-use mobile app (iOS/ Android) that connects to your PosiTector Advanced, PosiTector Smartlink, or PosiTest AT-A. Compatible with PosiSoft.net.

Learn More

PosiSoft USB

A simple gage interface to retrieve data in a manner similar to a flash drive. No software to install or internet connection required.

Learn More

PosiSoft Custom PDF Report Generator

featured on PosiSoft Desktop, PosiSoft.net, PosiTector App
Easily create reports from your measurement data in seconds
  • Generate custom, professional PDF reports
  • Include inspection information such as on-site pictures, screen captures, notes and more to communicate important details
  • Create and save multiple custom layouts as templates – insert cover pages, add logos/images, and select font and point size
  • Select the information to include for each product type – charts, histograms, readings, time stamps and more
  • Compile multi-batch reports from one or more probes and instrument types

PosiSoft.net

PosiSoft.net is a free cloud-based application offering secure storage of PosiTector and PosiTest Inspection Instrument data. Click Here to learn more.

PosiTector Developer Resources

From wired USB to WiFi wireless technology, DeFelsko instruments offer data management solutions for even the most advanced software integrations. Accessing your stored or live streaming data is simpler and more flexible than ever before. PosiTector and PosiTest AT-A instruments have the ability to integrate with third-party software, drones, ROVs, PLCs, and robotic devices using several industry-standard communication protocols.

Learn More about Integrating Third-Party Devices and Applications

F.A.Q.

plus-icon
minus-icon

Do your instruments require any formal training for use? Do you offer ‘demo’ models?

No. Our instruments are designed for simple operation, feature easy-to-use menus, instruction manuals, and helpful videos. In lieu of demonstration models, we provide unlimited technical support via telephone and/or email, and a limited 30-day money back guarantee.

plus-icon
minus-icon

Is the PosiTector 200 calibrated at the factory?

The PosiTector 200 arrives fully calibrated and ready to measure. A Long-Form Certificate of Calibration traceable to NIST or PTB is included, which documents actual readings taken by your instrument at our calibration laboratory on standards traceable to a national metrology institute. Beware of ‘Certificates’ or ‘Certificates of Conformance’ offered by competitors. These typically do not include actual instrument readings, and are often insufficient to meet common quality requirements.

The PosiTector 200 is factory calibrated to measure most polymer coatings out of the box without calibration or adjustment. If required, a simple gage adjustment can be made to a coating sample of known thickness as close as possible in composition to the intended application. For best results, the thickness of the sample should be equal to or slightly greater than the maximum expected thickness of the coating to be measured.

plus-icon
minus-icon

Can the PosiTector 200 be used to measure coatings on metal substrates?

In many cases, yes! However, the following should be noted:

  • Metal Substrate Thickness: Because sound travels through metals approximately three times faster than it travels through most protective coatings, substrate thickness will largely determine the suitability of a particular coating thickness application for the PosiTector 200.

  • Gage Adjustment: Adjustment to the PosiTector 200 gage’s Hi Range to eliminate unwanted metal substrate back-wall echoes is typically required for improved measurement repeatability. This process of adjustment is simplified through the use of the PosiTector 200 Advanced gage’s Graphics Mode. Although a PosiTector 200 Standard gage model has the capability to accurately measure single coat applications and a total coating system thickness of multi-layer applications, we strongly recommend the use of a PosiTector 200 Advanced gage model for measurement on metal substrates.

  • Single Coat Applications: A minimum coating thickness of 13µm (0.5 mil) on a flat metal substrate with a minimum thickness of 1.25mm (50 mils) is usually required.

  • Multi-Layer Applications –
  1. Total thickness: In many circumstances, the total thickness of a multi-layer coating system over metal can be reliably measured. As in single coat applications, a minimum total coating system coating thickness of 13µm (0.5 mil) on a flat metal substrate with a minimum thickness of 1.25mm (50 mils) is usually required.

  2. Individual layers: The PosiTector 200 will measure the thickness of individual layers when each layer is thicker than 125µm (5 mils) and the metal substrate is thicker than 6mm (0.25”). A greater difference in the acoustic characteristics of each layer results in a greater likelihood of accurate individual layer measurement.

A PosiTector 6000 probe is generally recommended over a PosiTector 200 probe for measuring coating thickness on metal substrates because –

  • Lower cost
  • Larger selection of probes (none requiring the use of an ultrasonic couplant gel)
  • Greater accuracy
  • Unlike PosiTector 200 probes, adjustment is not required for most protective coating properties
  • Fully conform to international standards for measuring coating thickness over metal
plus-icon
minus-icon

What is couplant? Do I need to use it every time I take a reading?

Couplant is required for every reading in order to propagate ultrasound into the coating. Water is a suitable couplant for smooth coatings. Use the supplied glycol gel for rougher coatings.

plus-icon
minus-icon

Can the PosiTector 200 measure coatings that contain particles or aggregate?

Broadcast epoxy, urethane mortar and other coating systems that contain aggregates or particulate inclusions (silica, quartz flake, concrete, etc.) will present a significant measurement challenge to our ultrasonic PosiTector 200 instrument. This is caused by the tendency of the solid particles to interfere with the ultrasonic impulse and typically results in unreliable thickness readings.

plus-icon
minus-icon

How do I ‘Zero’ the PosiTector 200?

Unlike a magnetic or eddy-current principle gage, an uncoated substrate is not required to Zero the PosiTector 200. Instead, the probe is held in the air away from the substrate when the Zero is performed.

plus-icon
minus-icon

How often should the PosiTector probe be recalibrated?

PosiTector probes include a Certificate of Calibration showing traceability to NIST or PTB included (Long Form) with each probe—with no expiry or end date. They have no shelf life, therefore the length of time in the field is not a good indicator for recalibration intervals. Many organizations with quality programs and recertification programs require annual recalibrations, and this is a good starting point for most users. DeFelsko recommends that customers establish calibration intervals based upon their own experience and work environment. Based on our product knowledge, data and customer feedback, a one year calibration interval from the date the instrument was placed in service is a good starting point.

plus-icon
minus-icon

Still need help?

Before returning your gage or instrument for service, review the troubleshooting steps on the Troubleshooting guide, or speak with a member of our technical support team by calling +1-315-393-4450.

Accessories

PosiTector Gage BodiesPosiTector Gage Bodies

PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.

Learn MoreLearn More
PosiTector ProbesPosiTector Probes

PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.

Learn MoreLearn More
Bluetooth PrinterBluetooth Printer

Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.

Learn MoreLearn More
Certified Thickness StandardsCertified Thickness Standards

Verify accuracy/operation of coating thickness gages. Important component of fulfilling both ISO/QS-9000 and in-house quality control requirements with a measurement accuracy traceable to NIST or PTB.

Learn MoreLearn More
PosiTector CasePosiTector Case

Convenient hard shell case for carrying a PosiTector gage body and multiple probes

Learn MoreLearn More
Certified Plastic ShimsCertified Plastic Shims

Economical alternative to Coated Metal Plates, with a reduced accuracy. Ideal for protecting the PosiTector probe tip.

Learn MoreLearn More
AC Power KitAC Power Kit

Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.

Learn MoreLearn More
Pelican Cases for PosiTector Inspection KitsPelican Cases for PosiTector Inspection Kits

Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTector instrument.

Learn MoreLearn More
Ultrasonic CouplantUltrasonic Couplant

Every PosiTector 200 and PosiTector UTG ships with (1) bottle of Ultrasonic couplant.  Additional 4oz. bottles are available (sold in case of 12 or twin packs).

Learn MoreLearn More
Belt ClipBelt Clip

Belt Clip for PosiTector gage bodies

Learn MoreLearn More
Certified Polystyrene BlocksCertified Polystyrene Blocks

Certified Polystyrene Blocks are for use with gages that measure over 1500 µm (60 mils).

Learn MoreLearn More
Non-Certified Plastic ShimsNon-Certified Plastic Shims

Provide a quick operational check of the instrument by allowing the user to perform practice measurements

Learn MoreLearn More
Protective Lens ShieldProtective Lens Shield

Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.

Learn MoreLearn More
View More Accessories

Resources

Downloads

Information