uparrow-iconp0chonk

PosiTest® AT

Pull-off Adhesion Testers

Measures adhesion of coatings to metal, wood, concrete and other rigid substrates.

  • Select from four Stand-offs - 20 mm, 50 mm, 50x50 mm Tile and 50 mm C1583
  • Environmentally sealed enclosure—weatherproof, dustproof and shockproof—meets or exceeds IP65
  • Inexpensive, single-use dollies eliminate cleaning for re-use and can be kept as a permanent record
  • Self-aligning aluminum dolly enables accurate measurements on smooth or uneven surfaces
  • 10, 14, 20 or 50 mm dollies maximize capability and measurement resolution across a wide range of bond strengths
  • Calibrated and certified to ± 1% accuracy using a NIST traceable load cell
  • Certificate of Calibration showing traceability to NIST included (Long Form)
Conforms to international standards including ASTM C1583/C1857/D4541/D7234/D7522, ISO 4624/16276-1,
EN 1542/12004-2, AS/NZS 1580.408.5 and others

Features

simple icon

Simple

  • Easily select dolly sizes, change measurement units, or store readings with the touch of a button
  • Inexpensive, single-use dollies and plates eliminate cleaning for re-use and can be kept as a permanent record
  • Each kit comes with everything needed for testing
durable icon

Durable

  • Environmentally sealed enclosure—weatherproof, dustproof and shockproof - meets or exceeds IP65
  • Hard-shell carrying case included, with optional upgrade to a heavy-duty Pelican case (Automatic models only)
  • Two year warranty
accurate icon

Accurate

  • Calibrated and certified to ± 1% accuracy using a NIST traceable load cell
  • Certificate of Calibration showing traceability to NIST included
  • Self-aligning dolly enables accurate measurements on smooth or uneven surfaces
  • Conforms to national and international standards including ASTM C1583/ C1857/ D4541/D7234/D7522, ISO 4624/16276-1, BS EN 12004-2, AS/NZS 1580.408.5, and others
accurate icon

Versatile

  • Select from four stand-offs to suit nearly any application
  • Internal memory stores maximum pull-off pressure, rate of pull, test duration, and dolly size
  • 10 mm, 14 mm, 20 mm, 50 mm, 50 x 50 mm Tile, and 50 mm C1583 dollies maximize capability and measurement resolution across a wide range of bond strengths
accurate icon

Powerful

PosiTest AT-A Automatic

PosiTest AT Automatic
See More Details
  • Electronically controlled hydraulic pump automatically applies smooth and continuous pull-off pressure. Greatly reduces user effort and the risk of influencing the pulling process
  • User adjustable pull rate, pull limit and hold time
  • Internal memory stores maximum pull-off pressure, rate of pull, test duration, pressure vs. time data, dolly size, pass/fail, nature of fracture and user notes for 100,000 pulls in up to 1,000 batches
  • Impact and scratch resistant color touch screen with keypad for operation with or without gloves
  • Compatible with PosiSoft Desktop, PosiSoft.net and PosiTector App (Apple iOS and Android)

PosiTest AT-M Manual

PosiTest AT Manual
See More Details
  • Manual hydraulic pump designed to apply smooth and continuous pressure with a single stroke
  • Pull Rate Indicator to manually monitor and adjust the rate of pull
  • Internal memory stores maximum pull-off pressure, rate of pull, test duration and dolly size for up to 200 pulls
  • Compatible with PosiSoft Desktop for viewing, printing and storing measurement data

PosiTest AT-A

Key Features...

  • Electronically controlled hydraulic pump automatically applies smooth and continuous pull-off pressure. Greatly reduces user effort and the risk of influencing the pulling process
  • Impact and scratch resistant color touch screen with keypad for operation with or without gloves
  • NEW Built-in Li-ion battery performs over 250 tests per charge.
  • NEW USB-C Port enables fast battery charging while simultaneously powering the instrument for uninterrupted use
  • Environmentally sealed enclosure—weatherproof, dustproof and shockproof—meets or exceeds IP65
  • Rubberized, shock absorbing grips provide a stable, skid-resistant footing
  • Self-aligning aluminum dolly enables accurate measurements on smooth or uneven surfaces
  • 10, 14, 20 or 50 mm dollies maximize capability and measurement resolution across a wide range of bond strengths. Maximum pull-off pressure by dolly size...
    - 10 mm: 14000 psi (96 MPa)
    - 14 mm: 7000 psi (50 MPa)
    - 20 mm: 3500 psi (24 MPa)
    - 50 mm: 560 psi (3.8 MPa)
  • User selectable measurement units: psi (pounds per square inch), MPa (Megapascal), Nmm2 (Newtons per millimeter square) or Newton (force)
  • User adjustable pull rate, pull limit and hold time
  • Rotating display for horizontal and vertical use
  • Calibrated and certified to ± 1% accuracy using a NIST traceable load cell

4 Automatic Models Available

Order Code
ATA20
ATA50

ATA50T

(EN 12004-2)

50x50 mm

ATA50C

(ASTM C1583 and EN 1542)

Dolly size and stand-off*
20 mm
50 mm
50 mm
Typical Applications
Higher bond strength coatings on metals
Lower bond strength coatings on wood, concrete and plastic
Concrete surfaces and overlays
Cementitious adhesives for tiles
Range
0.7 – 24 MPa
100 – 3500 psi
220 – 7550 N
0.1 – 3.8 MPa
16 – 560 psi
220 – 7550 N
0.1 – 3.0 MPa
13 – 440 psi
220 – 7550 N
0.1 – 3.8 MPa
16 – 560 psi
220 – 7550 N
Resolution
0.01 MPa (1 psi)
Accuracy
±1% Full Scale
Included Dollies
Ø20 mm (qty 20)
Aluminum
Ø50 mm (qty 8)
Aluminum
50x50 mm Plate (qty 4) with threaded post
Steel
Ø50 mm (qty 4)
with ≥ 25 mm thickness
Steel
Cutting Tool
20 mm hole saw
50 mm hole saw
-----
50 mm diamond grit hole saw with arbor

Adhesion testers include everything needed for testing: Automatic Adhesion Tester, built-in rechargeable Li-ion battery with charger, dollies, abrasive pad, cutting tool, glue with mixing sticks and palettes, cotton swabs, USB cable, PosiSoft Software, instruction booklet, shoulder strap, Certificate of Calibration traceable to NIST, two-year warranty, and a sturdy, lightweight carrying case^

* Optional 20mm/50mm/50 mm C1583/50 mm Tile Conversion Kits allow each model to be used with alternative dolly sizes. Custom 10 and 14 mm dollies are available for special applications (compatible with 20 mm stand off).

^ Upgrade to the Pelican® case by adding a '-P' to the Ordering Code.

Conforms to international standards including ASTM C1583/D4541/D7234/D7522, ISO 4624/16276-1, EN 1542/12004-2, AS/NZS 1580.408.5 and others

Memory and Reporting Features

  • Internal memory stores maximum pull-off pressure, rate of pull, test duration, pressure vs. time, dolly size, pass/fail, the nature of fracture, and notes for 100,000 pulls in up to 1,000 batches
  • Record the results as pass/fail and the nature of fracture - cohesive, adhesive and glue failures
  • Wirelessly connect to your smart device using our free PosiTector App (Apple iOS and Android)
  • WiFi technology wirelessly communicates with PosiSoft.net, downloads software updates and allows access to stored measurement data using standard web browsers (see WiFi Features for full details)
  • PosiSoft USB Drive—stored readings and graphs can be accessed via USB using universal PC/Mac web browsers or file explorers. No software required
  • Compatible with PosiSoft Desktop, PosiSoft.net and PosiTector App (Apple iOS and Android) software solutions

PosiTector App Features

PosiTector App in hand
  • Add images and notes using the camera or keyboard
  • Create customized, professional PDF reports
  • Share, backup, synchronize and report measurement data
  • Auto-pairing Bluetooth (BLE) connection
  • See the Help File to learn about how it works

Touch Screen Display

AT-A touch screen
Use the touch screen to interact with menu options. Swipe horizontally to navigate between views or vertically to move between batch readings. Alternatively, the keypad can be used for navigation and selection.
screenshot of AT-A screen during use
User adjustable dolly size, pull rate, 
pull limit and hold time.
screenshot of AT-A screen during use
Batch summary provides an at-a-glance review of test results.
screenshot of AT-A screen during use
View test parameters and reading results. Reading is recorded as pass or fail based on set test parameters. The pass/fail results can be revised.
screenshot of AT-A screen during use
Notes can be added for each reading.
screenshot of AT-A screen during use
Include a note for a batch (group) of readings.
screenshot of AT-A screen during use
Record the nature of failure—cohesive, adhesive and glue failures.

Recording the Nature of the Fracture

Upon completion of a pull-off test, the dolly and coated surface should be examined. In addition to pull-off force, many National and International standards such as ASTM D4541 and ISO 4624 require the nature of the fracture to be recorded.

‍

  • Cohesive fracture: fracture occurs within a coating layer (same coating on dolly face and coated surface).
  • Adhesive fracture: fracture occurs at the interface between layers (coating on dolly face differs from surface).
  • Glue failure: visible separation of the glue from itself, the coating or dolly (no coating visible on the dolly face).

‍

The cohesive and adhesive fracture visual analysis can be recorded using the PosiTest AT-A's keypad or touch screen display. Alternatively, the information can be reported using the PosiTector App.

Fractures are visually estimated and recorded as a percent of each. The two layer example below illustrates a cohesive fracture within coating layer 1 and layer 2 (visually estimated at 50% each). Recorded results are included in reports.

The PosiTest AT-A can record fracture information for up to five layers. For full details and examples see Visual Analysis and Recording of Test Results.

fracture types
fracture type explanations with screenshot of touch screen
See More Information

PosiTest AT-M

Key Features...

  • Manual hydraulic pump designed to apply smooth and continuous pressure with a single stroke
  • NEW High-contrast, easy to read color display
  • Environmentally sealed enclosure—weatherproof, dustproof and shockproof—meets or exceeds IP65
  • Self-aligning aluminum dolly enables accurate measurements on smooth or uneven surfaces
  • Pull Rate Indicator to manually monitor and adjust the rate of pull
  • Internal memory stores maximum pull-off pressure, pull rate, test duration and dolly size for up to 200 pulls
  • NEW Field replaceable AAA alkaline batteries provide up to 16 hours of testing
  • 10, 14, 20 or 50 mm dollies maximize capability and measurement resolution across a wide range of bond strengths
    - 10 mm: 10000 psi (70 MPa)
    - 14 mm: 6000 psi (40 MPa)
    - 20 mm: 3000 psi (20 MPa)
    - 50 mm: 480 psi (3.3 MPa)
    - 50x50 mm: 375 psi (2.585 MPa)
  • User selectable measurement units: psi (pounds per square inch) or MPa (Megapascal)
  • Every PosiTest Adhesion Tester is calibrated and certified to ± 1% accuracy using a NIST traceable load cell
  • Compatible with PosiSoft Desktop software for viewing, printing and storing measurement data

4 Manual Models Available

Order Code
ATM20
ATM50

ATM50T

(EN 12004-2)

50x50 mm

ATM50C

(ASTM C1583 and EN 1542)

Dolly size and stand-off*
20 mm
50 mm
50 mm
Typical Applications
Higher bond strength coatings on metals
Lower bond strength coatings on wood, concrete and plastic
Concrete surfaces and overlays
Cementitious adhesives for tiles
Range
0.7 – 20 MPa
100 – 3000 psi
0.1 – 3.3 MPa
16 – 480 psi
0.1 – 2.585 MPa
13 – 375 psi
0.1 – 3.3 MPa
16 – 480 psi
Resolution
0.01 MPa (1 psi)
Accuracy
±1% Full Scale
Included Dollies
Ø20 mm (qty 20)
Aluminum
Ø50 mm (qty 8)
Aluminum
50x50 mm Plate (qty 4) with threaded post
Steel
Ø50 mm (qty 4)
with ≥ 25 mm thickness
Steel
Cutting Tool
20 mm hole saw
50 mm hole saw
-----
50 mm diamond grit hole saw with arbor

Adhesion testers include everything needed for testing: Manual Adhesion Tester, 3 AAA batteries, dollies, abrasive pad, cutting tool, glue with mixing sticks and palettes, cotton swabs, USB cable, PosiSoft Software, instruction booklet, Certificate of Calibration traceable to NIST, two-year warranty, and a sturdy, lightweight carrying case

* Optional 20mm/50mm/50 mm C1583/50 mm Tile Conversion Kits allow each model to be used with alternative dolly sizes. Custom 10 and 14 mm dollies are available for special applications (compatible with 20 mm stand off).

Conforms to international standards including ASTM C1583/C1857/D4541/D7234/D7522, ISO 4624/16276-1, EN 1542/12004-2, AS/NZS 1580.408.5 and others

See More Information

Models

Step 1: Choose Manual or Automatic

Step 2: Choose Application

Image of the PosiTest ATM with the 20 mm actuator for use on coatings on metal
ATM20
Dolly size & Standoff
20 mm
Typical Applications
Coatings on
Metal
Range
0.7 - 20 MPa
100 - 3000 psi
View PDFAdd to Instant Quote
Image of the PosiTest ATM with the 50 mm actuator for use on coatings on concrete, wood, and plastic
ATM50
Dolly size & Standoff
50 mm
Typical Applications
Coatings on Concrete, Wood and Plastic
Range
0.1 - 3.5 MPa
16 - 480 psi
View PDFAdd to Instant Quote
Image of the PosiTest ATM with the 50 x 50 mm actuator for Tile Adhesion Strength testing, conforming to EN 12004-2
ATM50T
Dolly size & Standoff
50 x 50 mm
Typical Applications
Tile Adhesion Strength
Conforms to EN 12004-2
Range
0.1 - 2.585 MPa
13 - 375 psi
View PDFAdd to Instant Quote
Image of the PosiTest ATM with the 50 mm actuator for use on Concrete Surfaces and overlays that conform to ASTM C1583 and EN 1542
ATM50C
Dolly size & Standoff
50 mm
Typical Applications
Concrete Surfaces and Overlay
Conforms to ASTM C1583 and EN 1542
Range
0.1 - 3.5 MPa
16 - 480 psi
View PDFAdd to Instant Quote

Step 2: Choose Application

ATA20-420x258
ATA20
Dolly size & Standoff
20 mm
Typical Applications
Coatings on
Metal
Range
0.7 - 24 MPa
100 - 3500 psi
220 - 7550 N
View PDFAdd to Instant Quote
ATA50
Dolly size & Standoff
50 mm
Typical Applications
Coatings on Concrete, Wood
and Plastic
Range
0.1 - 3.8 MPa
16 - 560 psi
220 - 7550 N
View PDFAdd to Instant Quote
ATA50T
Dolly size & Standoff
50 x 50 mm
Typical Applications
Tile Adhesion Strength
Conforms to EN 12004-2
Range
0.4 - 3.033 MPa
50 - 440 psi
220 - 7550 N
View PDFAdd to Instant Quote
ATA50C
Dolly size & Standoff
50 mm
Typical Applications
Concrete Surfaces and Overlays
Conforms to ASTM C1583 and EN 1542
Range
0.4 - 3.8 MPa
50 - 560 psi
220 - 7550 N
View PDFAdd to Instant Quote

Videos

Video Thumbnail
PosiTest AT Probadores de Adherencia - Español
Video Thumbnail
How to Measure Adhesion Using the PosiTest AT Adhesion Tester
Video Thumbnail
PosiTest AT Self-Alignment Feature

Accessories

DolliesDollies

Loading fixtures, stubs for adhesion testing.

Learn MoreLearn More
PosiTest AT CalibratorPosiTest AT Calibrator

Ideal for verifying the accuracy and operation of PosiTest Adhesion Testers and is an important component in fulfilling both ISO and in-house quality control requirements.

Learn MoreLearn More
Pelican Case for PosiTest AT-A Pelican Case for PosiTest AT-A

Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTest instrument.

Learn MoreLearn More
50 mm C1583 Conversion Kit50 mm C1583 Conversion Kit

Interchangeable stand-off allows a PosiTest ATM or ATA to pull 50 mm dollies conforming to ASTM C1583. Ideal for concrete surfaces and overlays.

Learn MoreLearn More
50 mm x 50 mm Tile Conversion Kit50 mm x 50 mm Tile Conversion Kit

Interchangeable stand-off allows a PosiTest ATM or ATA to pull 50 mm x 50 mm square dollies conforming to BS EN 12004-2. Ideal for cementitious adhesive for tiles.

Learn MoreLearn More
50 mm Conversion Kit50 mm Conversion Kit

Interchangeable stand-off allows a PosiTest ATM20 or ATA20 to pull 50 mm dollies. Ideal for lower bond strength finishes such as coatings on wood, concrete and plastic.

Learn MoreLearn More
20 mm Conversion Kit20 mm Conversion Kit

Interchangeable stand-off allows a PosiTest ATM50 or ATA50 to pull 10, 14 and 20 mm dollies. Ideal for high bond strength finishes such as coatings on metal.

Learn MoreLearn More
Hole SawsHole Saws

Ideal for cutting or scoring through a coating around the edges of a dolly (pull stub) to isolate a specific diameter test area and remove excess glue, if required.

Learn MoreLearn More
Drilling Template for 50 mm DolliesDrilling Template for 50 mm Dollies

Drilling template and drill bits to isolate test area for pull-off adhesion tests, ideal for thicker coatings on concrete.

Learn MoreLearn More
Adhesive KitAdhesive Kit

Additional glue, mixing sticks, palettes and cotton swabs for pull-off adhesion tests

Learn MoreLearn More
View More Accessories

F.A.Q.

plus-icon
minus-icon

Is the PosiTest AT portable, and suitable for use in the field?

Absolutely. With an environmentally-sealed, metal enclosure, heavy-duty hydraulic pump and a high grade industrial pressure sensor, both the Manual and Automatic PosiTest AT are built to last. Weatherproof, dustproof and shockproof, they can be used indoors, outdoors and in all types of weather (meets or exceeds IP 65).

For added utility and convenience, PosiTest AT-A Automatic models also include a handy shoulder strap and rubberized grips.

plus-icon
minus-icon

Does the PosiTest AT include steel loading fixtures (dollies)?

The PosiTest AT 20 mm and 50 mm (ATM20 and ATM50) kits are supplied with self-aligning dollies that are precision-manufactured from a strong and lightweight aluminum alloy (6061-T6) as a lower-cost alternative to steel loading fixtures.

The PosiTest AT 50 x 50 mm and PosiTest AT 50 mm C1583 (ATM50T and ATM50C) kits are supplied with self-aligning steel dollies that are precision-manufactured to comply with relevant standards.

DeFelsko steel and aluminum dollies are a single-use/consumable items and ideal for keeping a permanent visual record of testing.

plus-icon
minus-icon

Do you have a recommended adhesive for my particular application?

The ResinLab EP11HT epoxy adhesive supplied with the PosiTest AT is simple to use and suitable for testing a wide range of coating types.  In some instances, specialized coatings will require a more specialized adhesive.

plus-icon
minus-icon

Is the PosiTest AT-A more accurate than the PosiTest AT-M?

The certified accuracy of both PosiTest AT models is +/- 1%. However, the fully automatic design of the PosiTest AT-A provides improved measurement consistency by eliminating the potential for operator influence from the test process.

plus-icon
minus-icon

What is the difference between the 20mm and the 50mm loading fixtures?

The 50 mm dolly is commonly recommended for use with concrete, wood and composite substrates, and measures coatings with expected adhesion values between 50 psi and 560 psi (50 - 500 psi for AT-M models). The 20 mm dolly is recommended for testing coatings applied to metals or with expected adhesion values greater than 500 psi.

plus-icon
minus-icon

Can I use the PosiTest AT-A on curved surfaces?

Yes. Feedback from our customers is that the PosiTest AT gages are suitable for testing most internal or external pipe applications greater than 200 mm in diameter.  In such cases, the maximum glue gap between the surface of the 20 mm dolly and the coating is 0.5 mm. For smaller pipe diameters, depending on the expected pull-off strength of the coating, it may be possible to use a 10 mm or 14 mm dolly. External diameters can be decreased to as low as 50 mm and 100 mm, for the 10 mm and 14 mm dollies, respectively.

DeFelsko does not provide or support the use of curved dollies for adhesion testing. In addition to affecting the surface area used in calculating pull-off strengths and the direction of the force lines (creating unwanted shear forces), most adhesion testing standards specifically call for the use of flat dollies.

plus-icon
minus-icon

How many measurements can I take with the PosiTest AT-A on a single battery charge?

The built-in rechargeable Li-ion battery (replaceable) in the PosiTest AT-A can perform over 250 tests on a single charge. The USB-C Port enables fast battery charging while simultaneously powering the instrument for uninterrupted use.

plus-icon
minus-icon

What is the lowest adhesion strength that the PosiTest AT-A can measure?

When utilized with a 50mm diameter dolly, the PosiTest AT is in a priming state until reaching a priming pressure of 16 psi. It is only after the priming pressure is reached that the instrument begins calculating and displaying the pull rate.

While it is possible to obtain readings below this priming pressure with the AT-M model, the AT-A automatic does not allow the operator to build priming pressure very slowly and is therefore not suitable for use below the priming pressure.

Note that all reported adhesion values (including those obtained below the priming pressure) are subject to the PosiTest AT gage’s full-scale accuracy of ± 1% (± 30 psi, AT-M; ± 35 psi, AT-A).

plus-icon
minus-icon

Is there a faster curing adhesive than the epoxy supplied with the PosiTest AT?

The versatile epoxy adhesive supplied with the PosiTest AT reaches full cure within 24 – 48 hours. Operators who require faster cure times should evaluate other adhesives for their compatibility with both the coating being tested and our aluminum test dolly. Cyanoacrylate (‘super glue’) type adhesives are often sufficient for lower pull-off strengths.

plus-icon
minus-icon

What is the minimum substrate thickness needed to test with the PosiTest AT?

DeFelsko does not specify a minimum substrate thickness for testing with PosiTest AT Adhesion Testers. Adhesion results can be affected by deformation of the substrate, which depends on factors such as material composition, thickness, and applied pulling force.

ISO 16276 recommends performing pull-off adhesion testing on steel substrates with a minimum of 3 mm (~1/8") to reduce the risk of deformation. When testing on thinner substrates, users should secure the part to a backing fixture or take other precautions to avoid bending or flexing of the material during the test.

Ultimately, the determination of minimum thickness should be made by the user based on the material properties, expected pull forces, coating system, and applicable test standards or specifications.

‍

plus-icon
minus-icon

Can I use the PosiTest AT on flexible or brittle substrates?

The PosiTest AT is designed for use with rigid, structural substrates. A flexible substrate can adversely impact test accuracy and repeatability. Furthermore, use of the PosiTest AT for measuring the adhesion of coatings applied to a brittle substrate typically results in the destruction of the substrate material, making it challenging to quantify the coating-substrate bond strength.

plus-icon
minus-icon

Is the PosiTest AT calibrated at the factory?

The PosiTest AT arrives fully calibrated and ready to measure. A Long-Form Certificate of Calibration traceable to NIST or PTB is included, which documents actual readings taken by your instrument at our calibration laboratory on standards traceable to a national metrology institute. Beware of ‘Certificates’ or ‘Certificates of Conformance’ offered by competitors. These typically do not include actual instrument readings, and are often insufficient to meet common quality requirements.

plus-icon
minus-icon

Do your instruments require any formal training for use? Do you offer ‘demo’ models?

No. Our instruments are designed for simple operation, feature easy-to-use menus, instruction manuals, and helpful videos. In lieu of demonstration models, we provide unlimited technical support via telephone and/or email, and a limited 30-day money back guarantee.

plus-icon
minus-icon

Still need help?

Before returning your gage or instrument for service, review the troubleshooting steps on the Troubleshooting guide, or speak with a member of our technical support team by calling +1-315-393-4450.

Software

PosiSoft Software in use

PosiSoft Desktop

Powerful desktop software for downloading, archiving, and reporting measurement data. No internet connection required.

  • Simple, intuitive user interface
  • Import readings directly from the gage via USB, WiFi, or legacy PosiSoft Desktop versions
  • Fully integrates with PosiSoft.net—backup and synchronize jobs, batches, readings, and report templates to the cloud. Click here to learn more about PosiSoft.net
Learn More

PosiTector App

An easy-to-use mobile app (iOS/ Android) that connects to your PosiTector Advanced, PosiTector Smartlink, or PosiTest AT-A. Compatible with PosiSoft.net.

Learn More

PosiSoft USB

A simple gage interface to retrieve data in a manner similar to a flash drive. No software to install or internet connection required.

Learn More

PosiSoft Custom PDF Report Generator

featured on PosiSoft Desktop, PosiSoft.net, PosiTector App
Easily create reports from your measurement data in seconds
  • Generate custom, professional PDF reports
  • Include inspection information such as on-site pictures, screen captures, notes and more to communicate important details
  • Create and save multiple custom layouts as templates – insert cover pages, add logos/images, and select font and point size
  • Select the information to include for each product type – charts, histograms, readings, time stamps and more
  • Compile multi-batch reports from one or more probes and instrument types

PosiSoft.net

PosiSoft.net is a free cloud-based application offering secure storage of PosiTector and PosiTest Inspection Instrument data. Click Here to learn more.

PosiTector Developer Resources

From wired USB to WiFi wireless technology, DeFelsko instruments offer data management solutions for even the most advanced software integrations. Accessing your stored or live streaming data is simpler and more flexible than ever before. PosiTector and PosiTest AT-A instruments have the ability to integrate with third-party software, drones, ROVs, PLCs, and robotic devices using several industry-standard communication protocols.

Learn More about Integrating Third-Party Devices and Applications

Resources

Downloads

Information