ATA50T
(EN 12004-2)
ATA50C
(ASTM C1583 and EN 1542)
Adhesion testers include everything needed for testing: Automatic Adhesion Tester, built-in rechargeable Li-ion battery with charger, dollies, abrasive pad, cutting tool, glue with mixing sticks and palettes, cotton swabs, USB cable, PosiSoft Software, instruction booklet, shoulder strap, Certificate of Calibration traceable to NIST, two-year warranty, and a sturdy, lightweight carrying case^
* Optional 20mm/50mm/50 mm C1583/50 mm Tile Conversion Kits allow each model to be used with alternative dolly sizes. Custom 10 and 14 mm dollies are available for special applications (compatible with 20 mm stand off).
^ Upgrade to the Pelican® case by adding a '-P' to the Ordering Code.
Conforms to international standards including ASTM C1583/D4541/D7234/D7522, ISO 4624/16276-1, EN 1542/12004-2, AS/NZS 1580.408.5 and others
.png)







Upon completion of a pull-off test, the dolly and coated surface should be examined. In addition to pull-off force, many National and International standards such as ASTM D4541 and ISO 4624 require the nature of the fracture to be recorded.
The cohesive and adhesive fracture visual analysis can be recorded using the PosiTest AT-A's keypad or touch screen display. Alternatively, the information can be reported using the PosiTector App.
Fractures are visually estimated and recorded as a percent of each. The two layer example below illustrates a cohesive fracture within coating layer 1 and layer 2 (visually estimated at 50% each). Recorded results are included in reports.
The PosiTest AT-A can record fracture information for up to five layers. For full details and examples see Visual Analysis and Recording of Test Results.


ATM50T
(EN 12004-2)
ATM50C
(ASTM C1583 and EN 1542)
Adhesion testers include everything needed for testing: Manual Adhesion Tester, 3 AAA batteries, dollies, abrasive pad, cutting tool, glue with mixing sticks and palettes, cotton swabs, USB cable, PosiSoft Software, instruction booklet, Certificate of Calibration traceable to NIST, two-year warranty, and a sturdy, lightweight carrying case
* Optional 20mm/50mm/50 mm C1583/50 mm Tile Conversion Kits allow each model to be used with alternative dolly sizes. Custom 10 and 14 mm dollies are available for special applications (compatible with 20 mm stand off).
Conforms to international standards including ASTM C1583/C1857/D4541/D7234/D7522, ISO 4624/16276-1, EN 1542/12004-2, AS/NZS 1580.408.5 and others








Ideal for verifying the accuracy and operation of PosiTest Adhesion Testers and is an important component in fulfilling both ISO and in-house quality control requirements.
Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTest instrument.
Interchangeable stand-off allows a PosiTest ATM or ATA to pull 50 mm dollies conforming to ASTM C1583. Ideal for concrete surfaces and overlays.
Interchangeable stand-off allows a PosiTest ATM or ATA to pull 50 mm x 50 mm square dollies conforming to BS EN 12004-2. Ideal for cementitious adhesive for tiles.
Interchangeable stand-off allows a PosiTest ATM20 or ATA20 to pull 50 mm dollies. Ideal for lower bond strength finishes such as coatings on wood, concrete and plastic.
Interchangeable stand-off allows a PosiTest ATM50 or ATA50 to pull 10, 14 and 20 mm dollies. Ideal for high bond strength finishes such as coatings on metal.
Ideal for cutting or scoring through a coating around the edges of a dolly (pull stub) to isolate a specific diameter test area and remove excess glue, if required.
Drilling template and drill bits to isolate test area for pull-off adhesion tests, ideal for thicker coatings on concrete.
Additional glue, mixing sticks, palettes and cotton swabs for pull-off adhesion tests
Absolutely. With an environmentally-sealed, metal enclosure, heavy-duty hydraulic pump and a high grade industrial pressure sensor, both the Manual and Automatic PosiTest AT are built to last. Weatherproof, dustproof and shockproof, they can be used indoors, outdoors and in all types of weather (meets or exceeds IP 65).
For added utility and convenience, PosiTest AT-A Automatic models also include a handy shoulder strap and rubberized grips.
The PosiTest AT 20 mm and 50 mm (ATM20 and ATM50) kits are supplied with self-aligning dollies that are precision-manufactured from a strong and lightweight aluminum alloy (6061-T6) as a lower-cost alternative to steel loading fixtures.
The PosiTest AT 50 x 50 mm and PosiTest AT 50 mm C1583 (ATM50T and ATM50C) kits are supplied with self-aligning steel dollies that are precision-manufactured to comply with relevant standards.
DeFelsko steel and aluminum dollies are a single-use/consumable items and ideal for keeping a permanent visual record of testing.
The ResinLab EP11HT epoxy adhesive supplied with the PosiTest AT is simple to use and suitable for testing a wide range of coating types. In some instances, specialized coatings will require a more specialized adhesive.
The certified accuracy of both PosiTest AT models is +/- 1%. However, the fully automatic design of the PosiTest AT-A provides improved measurement consistency by eliminating the potential for operator influence from the test process.
The 50 mm dolly is commonly recommended for use with concrete, wood and composite substrates, and measures coatings with expected adhesion values between 50 psi and 560 psi (50 - 500 psi for AT-M models). The 20 mm dolly is recommended for testing coatings applied to metals or with expected adhesion values greater than 500 psi.
Yes. Feedback from our customers is that the PosiTest AT gages are suitable for testing most internal or external pipe applications greater than 200 mm in diameter. In such cases, the maximum glue gap between the surface of the 20 mm dolly and the coating is 0.5 mm. For smaller pipe diameters, depending on the expected pull-off strength of the coating, it may be possible to use a 10 mm or 14 mm dolly. External diameters can be decreased to as low as 50 mm and 100 mm, for the 10 mm and 14 mm dollies, respectively.
DeFelsko does not provide or support the use of curved dollies for adhesion testing. In addition to affecting the surface area used in calculating pull-off strengths and the direction of the force lines (creating unwanted shear forces), most adhesion testing standards specifically call for the use of flat dollies.
The built-in rechargeable Li-ion battery (replaceable) in the PosiTest AT-A can perform over 250 tests on a single charge. The USB-C Port enables fast battery charging while simultaneously powering the instrument for uninterrupted use.
When utilized with a 50mm diameter dolly, the PosiTest AT is in a priming state until reaching a priming pressure of 16 psi. It is only after the priming pressure is reached that the instrument begins calculating and displaying the pull rate.
While it is possible to obtain readings below this priming pressure with the AT-M model, the AT-A automatic does not allow the operator to build priming pressure very slowly and is therefore not suitable for use below the priming pressure.
Note that all reported adhesion values (including those obtained below the priming pressure) are subject to the PosiTest AT gage’s full-scale accuracy of ± 1% (± 30 psi, AT-M; ± 35 psi, AT-A).
The versatile epoxy adhesive supplied with the PosiTest AT reaches full cure within 24 – 48 hours. Operators who require faster cure times should evaluate other adhesives for their compatibility with both the coating being tested and our aluminum test dolly. Cyanoacrylate (‘super glue’) type adhesives are often sufficient for lower pull-off strengths.
DeFelsko does not specify a minimum substrate thickness for testing with PosiTest AT Adhesion Testers. Adhesion results can be affected by deformation of the substrate, which depends on factors such as material composition, thickness, and applied pulling force.
ISO 16276 recommends performing pull-off adhesion testing on steel substrates with a minimum of 3 mm (~1/8") to reduce the risk of deformation. When testing on thinner substrates, users should secure the part to a backing fixture or take other precautions to avoid bending or flexing of the material during the test.
Ultimately, the determination of minimum thickness should be made by the user based on the material properties, expected pull forces, coating system, and applicable test standards or specifications.
The PosiTest AT is designed for use with rigid, structural substrates. A flexible substrate can adversely impact test accuracy and repeatability. Furthermore, use of the PosiTest AT for measuring the adhesion of coatings applied to a brittle substrate typically results in the destruction of the substrate material, making it challenging to quantify the coating-substrate bond strength.
The PosiTest AT arrives fully calibrated and ready to measure. A Long-Form Certificate of Calibration traceable to NIST or PTB is included, which documents actual readings taken by your instrument at our calibration laboratory on standards traceable to a national metrology institute. Beware of ‘Certificates’ or ‘Certificates of Conformance’ offered by competitors. These typically do not include actual instrument readings, and are often insufficient to meet common quality requirements.
No. Our instruments are designed for simple operation, feature easy-to-use menus, instruction manuals, and helpful videos. In lieu of demonstration models, we provide unlimited technical support via telephone and/or email, and a limited 30-day money back guarantee.
Before returning your gage or instrument for service, review the troubleshooting steps on the Troubleshooting guide, or speak with a member of our technical support team by calling +1-315-393-4450.
.png)
Powerful desktop software for downloading, archiving, and reporting measurement data. No internet connection required.
An easy-to-use mobile app (iOS/ Android) that connects to your PosiTector Advanced, PosiTector Smartlink, or PosiTest AT-A. Compatible with PosiSoft.net.
Learn MoreA simple gage interface to retrieve data in a manner similar to a flash drive. No software to install or internet connection required.
Learn More
PosiSoft.net is a free cloud-based application offering secure storage of PosiTector and PosiTest Inspection Instrument data. Click Here to learn more.
From wired USB to WiFi wireless technology, DeFelsko instruments offer data management solutions for even the most advanced software integrations. Accessing your stored or live streaming data is simpler and more flexible than ever before. PosiTector and PosiTest AT-A instruments have the ability to integrate with third-party software, drones, ROVs, PLCs, and robotic devices using several industry-standard communication protocols.
DeFelsko Corporation, a leading U.S. Manufacturer of coating thickness gages and inspection instruments, has been delivering Simple, Durable and Accurate gages since 1965. Family owned and operated in Northern New York, its state-of-the-art facility houses research, development, manufacturing, quality, sales, training and service departments.
Use the latest technological advances combined with over 60 years of experience to manufacture the most Simple, Durable, and Accurate inspection instruments.
With unequaled handling characteristics and easy, trouble-free operation. They are simple to use and employ leading-edge technology. They come complete with a 30-day money-back guarantee.

Unequal pulling force during testing caused by uneven adhesive bond lines and coating surfaces can result in random, unexplainable readings. To obtain more repeatable and meaningful adhesion measurements, it is imperative that the pulling force applied to the test dolly is uniformly distributed over the surface being tested.
Both the PosiTest AT-M manual and PosiTest AT-A automatic models compensate for misalignment. The self-aligning, quick-coupling actuator and spherical articulating dolly head enable uniform distribution of the pulling force over the surface being tested, preventing a one-sided pull-off.