uparrow-iconp0chonk

PosiTector® SST

Soluble Salt Tester for measuring the concentration of soluble salts on metal surfaces

The PosiTector SST Soluble Salt Tester measures the concentration of soluble salts (salt contamination) on metal surfaces in accordance with ISO 8502-6, 8502-9.

  • Conductivity probe specifically designed for ISO 8502-6, 9—the Bresle Method
  • Displays test duration, sample temperature, conductivity (µS/cm) and surface density (mg/m2 or µg/cm2)
  • Easy 1-2-3 gage interface guides users through the Bresle test method
  • Large 2.8" impact resistant color touchscreen with redesigned keypad for quick menu navigation
  • Weatherproof, dustproof, and water-resistant—IP65-rated enclosure
  • PosiTector interchangeable platform—attach any PosiTector probe to a single gage body
  • USB, WiFi, and Bluetooth connectivity to PosiSoft PC, Mac, and Smartphone software
  • Certificate of Calibration showing traceability to NIST included (Long Form)
Conforms to ISO 8502-6/8502-9, US Navy PPI 63101-000, U.S. Navy NAVSEA NSI 009-32, AS 3894.6, IMO MSC.215(82), IMO MSC.244(83), SSPC Guide 15, ISO 11127-6, ASTM D4940

Features

simple icon

Simple

  • Conductivity probe specifically designed for ISO 8502-6,9—the Bresle Method
  • Displays test duration, sample temperature, conductivity (µS/cm) and surface density (mg/m2 or µg/cm2)
  • Large 2.8" impact resistant color touchscreen with redesigned keypad for quick menu navigation
  • On-gage help explains menu items at the touch of a button
  • Easy 1-2-3 gage interface guides users through the Bresle test method
  • Automatic storage of a background (blank) measurement—handy when performing multiple salt tests
durable icon

Durable

  • Weatherproof, dustproof, and water-resistant—IP65-rated enclosure
  • Ergonomic design with durable rubberized grip
  • Shock-absorbing protective rubber holster for added impact resistance
  • Two year warranty on gage body AND probe
accurate icon

Accurate

  • Long Form Certificate of Calibration showing traceability to NIST included
  • Includes certified conductivity standard (calibration solution) to verify probe accuracy. Certificate included.
  • Automatic temperature normalization and sample temperature reporting
  • Conforms to ISO 8502-6/8502-9, US Navy NSI 009-32, US Navy PPI 63101-000, AS 3894.6, IMO MSC.215(82), IMO MSC.244(83), SSPC Guide 15, ISO 11127-6, ASTM D4940
versatile icon

Versatile

  • PosiTector body accepts all PosiTector 6000, 200, RTR, SPG, DPM, IRT, SST, UTG, SHD, BHI, and GLS probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, ultrasonic wall thickness gage, hardness tester, or gloss meter
  • Ideal for determination of water-soluble contaminants in non-metallic blast media
  • A selection of kits include everything needed to retrieve and analyze soluble salts on surfaces
  • Adjustable for various Bresle patch volumes
  • Selectable display languages
  • Auto rotating display with Flip Lock
powerful icon

Powerful

  • Track and record test duration in accordance with ISO 8502-6
  • Screen Capture—save 100 screen images for record keeping and review
  • Instant-on feature quickly powers up the gage if recently powered down
  • Over 20 hours of continuous operation with 3 AAA batteries
  • USB port for fast, simple connection to a PC and to supply continuous power. USB cable included
  • PosiSoft USB Drive—stored readings and graphs can be accessed using universal PC/Mac web browsers or file explorers. No software required.
  • Software Updates via web keep your gage current
  • Includes PosiSoft suite of software for viewing and reporting data
  • Every stored measurement is date and time stamped
specifications icon

Specifications

Range
0 – 1,500 μS/cm
0 – 6,000 mg/m2
0.0 – 600.0 μg/cm2
Resolution*
1 μS/cm, 1mg/m2, 0.1 μg/cm2
Accuracy
± 2 μS/cm (0 – 200 μS/cm)
± 10 μS/cm (>200 – 600 μS/cm)
± 20 μS/cm (>600 – 1500 μS/cm)
Temperature Range
0 – 50° C (32 – 122° F)
Normalization Temperature
25° C (77° F)
Test Cell Volume
1 ml
Size^
127 x 66 x 25.4 mm (5" x 2.6" x 1")
Weight^
137 g (4.9 oz.) without batteries
* Hi Res Mode increases resolution to 0.1 μS/cm (0 - 200 μS/cm)
^ Size and weight are for the PosiTector gage body only and do not include the probe.

Standard Models

Includes ALL features as shown on left plus...
Includes ALL features as shown above plus...
  • Storage of 1,000 readings per probe—stored readings can be viewed or downloaded

Advanced Models

Includes ALL features as shown on left plus...
Includes ALL features as shown above plus...
  • Storage of 250,000 readings from multiple probes in up to 1,000 batches
  • Touchscreen keyboard for quickly renaming batches, adding notes, and more
  • WiFi technology wirelessly synchronizes with PosiSoft.net and downloads software updates
  • Bluetooth 4.0 Technology for data transfer to a mobile device running the PosiTector App or optional portable printer. BLE API available for integration into third-party software.
  • Integrate with third-party software, drones, ROVs, PLCs, and robotic devices using several industry-standard communication protocols
View More Features

Bresle Test Method Patch Options

PosiPatch in use
PosiPatchTM

Reusable Bresle patch with Standard or Flexible magnetic ring—lowest per test cost

Learn More
DeFelsko Adhesive Patch in use
DeFelsko Adhesive Patch

Self-adhesive, polyurethane Bresle Test patches

Learn More
Latex Adhesive Patch in use
Latex Adhesive Patch

Latex Bresle Test patch with easy-open tabs and low-tack adhesive for easy removal

Learn More

Models

View PDF Order Guide 

Step 1: Choose a gage body

Step 2: Select A Model

Click model to download cutsheet
PosiTector SST
SST1
Inclusions
PosiTector Standard Gage Body
PosiTector SST Probe
---
---
---
---
Protective carrying case

View PDFAdd to Instant Quote
PosiTector SST PosiPatch standard gage kit
SSTKITP1
Inclusions
PosiTector Standard Gage Body
PosiTector SST Probe
PosiPatch (5)
Standard Magnetic Ring
Syringe and Plastic Tip (2)
250 ml DI Water
Cup (5)
Hard-shell Carrying Case
View PDFAdd to Instant Quote
PosiTector SST PosiPatch standard gage kit
SSTKITPF1
Inclusions
PosiTector Standard Gage Body
PosiTector SST Probe
PosiPatch (5)
Flexible Magnetic Ring
Syringe and Plastic Tip (2)
250 ml DI Water
Cup (5)
Hard-shell Carrying Case
View PDFAdd to Instant Quote
PosiTector SST adhesive patch standard gage kit
SSTKITD1
Inclusions
PosiTector Standard Gage Body
PosiTector SST Probe
DeFelsko Adhesive Patch (25)
---
Syringe and Needle (2)
250 ml DI Water
Cup (5)
Hard-shell Carrying Case
View PDFAdd to Instant Quote
PosiTector SST latex patch standard gage kit
SSTKITL1
Inclusions
PosiTector Standard Gage Body
PosiTector SST Probe
Latex Adhesive Patch (25)
---
Syringe and Needle (2)
250 ml DI Water
Cup (5)
Hard-shell Carrying Case
View PDFAdd to Instant Quote
PosiTector SST Standard/Advanced Body + Probe models come complete with: protective rubber holster, certified conductivity standard, foam swabs (5), Long Form Certificate of Calibration traceable to NIST, wrist strap, 3 AAA alkaline batteries, instructions, protective lens shield, USB cable, PosiSoft Software, two (2) year warranty.

Step 2: Choose material type

Click model to download cutsheet
PosiTector SST
SST3
Inclusions
PosiTector Advanced Gage Body
PosiTector SST Probe
---
---
---
---
Protective carrying case

View PDFAdd to Instant Quote
PosiTector SST PosiPatch standard gage kit
SSTKITP3
Inclusions
PosiTector Advanced Gage Body
PosiTector SST Probe
PosiPatch (5)
Standard Magnetic Ring
Syringe and Plastic Tip (2)
250 ml DI Water
Cup (5)
Hard-shell Carrying Case
View PDFAdd to Instant Quote
PosiTector SST PosiPatch standard gage kit
SSTKITPF3
Inclusions
PosiTector Advanced Gage Body
PosiTector SST Probe
PosiPatch (5)
Flexible Magnetic Ring
Syringe and Plastic Tip (2)
250 ml DI Water
Cup (5)
Hard-shell Carrying Case
View PDFAdd to Instant Quote
PosiTector SST adhesive patch standard gage kit
SSTKITD3
Inclusions
PosiTector Advanced Gage Body
PosiTector SST Probe
DeFelsko Adhesive Patch (25)
---
Syringe and Needle (2)
250 ml DI Water
Cup (5)
Hard-shell Carrying Case
View PDFAdd to Instant Quote
PosiTector SST latex patch standard gage kit
SSTKITL3
Inclusions
PosiTector Advanced Gage Body
PosiTector SST Probe
Latex Adhesive Patch (25)
---
Syringe and Needle (2)
250 ml DI Water
Cup (5)
Hard-shell Carrying Case
View PDFAdd to Instant Quote
PosiTector SST Standard/Advanced Body + Probe models come complete with: protective rubber holster, certified conductivity standard, foam swabs (5), Long Form Certificate of Calibration traceable to NIST, wrist strap, 3 AAA alkaline batteries, instructions, protective lens shield, USB cable, PosiSoft Software, two (2) year warranty.

Step 2: Choose material type

Click model to download cutsheet
PosiTector SST Probe
PRBSST
Inclusions
PosiTector SST probe only
---
---
---
---
---
View PDFAdd to Instant Quote
PosiTector SST probe only PosiPatch kit
SSTKITP
Inclusions
PosiTector SST Probe only
PosiPatch (5) 
Standard Magnetic Ring* 
Syringe and Plastic Tip (2) 
250 ml DI Water
Cup (5)
View PDFAdd to Instant Quote
PosiTector SST PosiPatch standard gage kit
SSTKITPF
Inclusions
PosiTector SST Probe only
PosiPatch (5) 
Flexible Magnetic Ring* 
Syringe and Plastic Tip (2) 
250 ml DI Water
Cup (5)
View PDFAdd to Instant Quote
PosiTector SST probe only adhesive patch kit
SSTKITD
Inclusions
PosiTector SST Probe only
DeFelsko Adhesive Patch (25)
---
Syringe and Needle (2)
250 ml DI Water
Cup (5)
View PDFAdd to Instant Quote
PosiTector SST probe only latex patch kit
SSTKITL
Inclusions
PosiTector SST Probe only
Latex Adhesive Patch (25)
---
Syringe and Needle (2)
250 ml DI Water
Cup (5)
View PDFAdd to Instant Quote
PosiTector SST Standard/Advanced Body + Probe models come complete with: protective rubber holster, certified conductivity standard, foam swabs (5), Long Form Certificate of Calibration traceable to NIST, belt clip, wrist strap, 3 AAA alkaline batteries, instructions, protective lens shield, USB cable, PosiSoft Software, two (2) year warranty.
Note: Newer probes may not be compatible with older gage bodies. See probe compatibility chart for more information

Videos

Video Thumbnail
How to Measure Salt Contamination with the PosiTector SST Soluble Salt Tester
Video Thumbnail
Saving Money and Time with PosiTector Probe Interchangeability
Video Thumbnail
New PosiTector Gage Body
Video Thumbnail
PosiTector SST Webinar
Video Thumbnail
DeFelsko Bresle Method Patches - Competitive Advantages

Software

PosiSoft Software in use

PosiSoft Desktop

Powerful desktop software for downloading, archiving, and reporting measurement data. No internet connection required.

  • Simple, intuitive user interface
  • Import readings directly from the gage via USB, WiFi, or legacy PosiSoft Desktop versions
  • Fully integrates with PosiSoft.net—backup and synchronize jobs, batches, readings, and report templates to the cloud. Click here to learn more about PosiSoft.net
Learn More

PosiTector App

An easy-to-use mobile app (iOS/ Android) that connects to your PosiTector Advanced, PosiTector Smartlink, or PosiTest AT-A. Compatible with PosiSoft.net.

Learn More

PosiSoft USB

A simple gage interface to retrieve data in a manner similar to a flash drive. No software to install or internet connection required.

Learn More

PosiSoft Custom PDF Report Generator

featured on PosiSoft Desktop, PosiSoft.net, PosiTector App
Easily create reports from your measurement data in seconds
  • Generate custom, professional PDF reports
  • Include inspection information such as on-site pictures, screen captures, notes and more to communicate important details
  • Create and save multiple custom layouts as templates – insert cover pages, add logos/images, and select font and point size
  • Select the information to include for each product type – charts, histograms, readings, time stamps and more
  • Compile multi-batch reports from one or more probes and instrument types

PosiSoft.net

PosiSoft.net is a free cloud-based application offering secure storage of PosiTector and PosiTest Inspection Instrument data. Click Here to learn more.

PosiTector Developer Resources

From wired USB to WiFi wireless technology, DeFelsko instruments offer data management solutions for even the most advanced software integrations. Accessing your stored or live streaming data is simpler and more flexible than ever before. PosiTector and PosiTest AT-A instruments have the ability to integrate with third-party software, drones, ROVs, PLCs, and robotic devices using several industry-standard communication protocols.

Learn More about Integrating Third-Party Devices and Applications

F.A.Q.

plus-icon
minus-icon

Why is salt contamination measurement important?

The presence of soluble salts has been shown to have a significant negative effect on coating performance and leads to premature coating failure. Salts remaining beneath a protective coating create an osmotic force that draws water from the atmosphere through the paint layer. The pressure created by this water underneath the coating overcomes the adhesive bond between the coating and substrate, resulting in corrosion, osmotic blistering, and eventual coating failure. It is therefore critical to ensure that a substrate is free from soluble salt contamination before painting.

plus-icon
minus-icon

What is measured with the PosiTector SST?

Includes a certified and traceable conductivity probe specifically designed for measuring soluble salts in accordance with ISO 8502-6,9—the Bresle Method (Salts Test). Included with each probe is a Long Form Certificate of Calibration. The following parameters are measured by the PosiTector SST:

  • Conductivity (µS/cm)
  • Sampling Temperature (C° or F°) normalized to 25°C
  • Test duration

Using the measured conductivity value and the sample test volume (set within the gage menu), the surface density of the salts (mg/m2 or µg/cm2) is automatically calculated in accordance with ISO 8502-9, saving the gage operator time and eliminating the chance of a calculation error.

plus-icon
minus-icon

What are some typical applications?

The PosiTector SST Soluble Salt Tester is ideal for: 

(a) Testing substrates for the presence of soluble salts in accordance with ISO 8502-6,9 (the Bresle Method)

(b) Testing blast media in accordance with ASTM 4940 and ISO 11127-6 (determination of water-soluble contaminates in abrasives by conductivity measurement)

(c) Testing the conductivity of water within the range of 0-500 µS/cm

plus-icon
minus-icon

How is the PosiTector SST conductivity probe different than the conventional conductivity meters included with most other test kits?

The PosiTector SST conductivity probe is specifically designed for testing soluble salts in accordance with ISO 8502-6,9 and has a number of features not found in conventional conductivity meters including . . .

  • An onscreen user interface to walk users through the Bresle test method, simplifying the task
  • Tracking and reporting of test duration (the total time of contact between the solvent and substrate) as required by ISO 8502-6
  • Automatic calculation of surface density with adjustments for different patch volumes – works with ANY Bresle-type patch
  • Free software for viewing and reporting data
  • Long form certificate of calibration traceable to NIST included at no extra charge. A certificate also comes with the included conductivity standard (calibration solution).
  • Automatic 25°C temperature normalization
  • Sample temperature recording as required by ISO 8502-9
  • Purpose-built, 1 ml test cell is optimized for the range, resolution and test volume of the Bresle Method
  • Rugged, stainless steel electrodes – ideal for industrial environments
  • Two year warranty
plus-icon
minus-icon

What information does the PosiTector SST save in its memory for each salts test?

The PosiTector SST Soluble Salt Tester saves all measured information for each salts test. All information can also be reported in PosiSoft software.

  • Date and time of test
  • Test duration (the total time of contact between the solvent and substrate)
  • Background sample temperature (°C or °F)
  • Final sample temperature (°C or °F)
  • Increase in conductivity between background and final sample (µS/cm)
  • Calculated surface density of soluble salts (mg NaCl/m2, mg CL/m2, µg NaCl/cm2, or µg Cl/cm2)
plus-icon
minus-icon

Does the PosiTector SST Soluble Salt Tester need to be calibrated prior to use?

The PosiTector SST Soluble Salt Tester arrives fully calibrated and ready to measure. A Long-Form Certificate of Calibration traceable to NIST or PTB is included, which documents actual readings taken by your conductivity probe at our calibration laboratory on standards traceable to a national metrology institute. Beware of ‘Certificates’ or ‘Certificates of Conformance’ offered by competitors. These typically do not include actual instrument readings, and are often insufficient to meet common quality requirements.

A Verification of Accuracy can be performed by measuring known reference standards such as the supplied conductivity standard.

plus-icon
minus-icon

Does the PosiTector SST measure the concentration of individual salt ions?

The PosiTector SST Soluble Salt Tester measures the overall conductivity of the test solution, and using calculations specified in ISO 8502-9, converts this value into a total surface density of salts.

plus-icon
minus-icon

Does the PosiTector SST display readings in PPM of salt?

The PosiTector SST Soluble Salt Tester is built specifically for the Bresle test method which does not address PPM calculations. While empirical conversion factors exist for converting PPM to surface density, these are not recognized by any test method.

plus-icon
minus-icon

Can the PosiTector SST probe be immersed in the fluid it is testing?

Yes. By immersing only the test cell, the PosiTector SST Soluble Salt Tester is ideal for testing the conductivity of water within the range of 0-500 µS/cm.

plus-icon
minus-icon

Can the PosiTector SST be used to measure the salt concentration in blast media?

Yes. The PosiTector SST Soluble Salt Tester can be used as a conventional conductivity meter making it ideal for testing abrasive materials in accordance with ISO 11127-6 and ASTM D4940-15.

plus-icon
minus-icon

How often should the PosiTector probe be recalibrated?

PosiTector probes include a Certificate of Calibration showing traceability to NIST or PTB included (Long Form) with each probe—with no expiry or end date. They have no shelf life, therefore the length of time in the field is not a good indicator for recalibration intervals. Many organizations with quality programs and recertification programs require annual recalibrations, and this is a good starting point for most users. DeFelsko recommends that customers establish calibration intervals based upon their own experience and work environment. Based on our product knowledge, data and customer feedback, a one year calibration interval from the date the instrument was placed in service is a good starting point.

plus-icon
minus-icon

What is a Bresle Test?

The Bresle Method Test, also known as a “salts test”, measures the concentration of soluble salts on steel surfaces prior to abrasive blast cleaning and paint application. The Bresle Method tests for salts by sampling a surface by means of “surface extraction”. Put simply, this method involves placing a volume of water in a chamber against the test surface. The water dissolves the soluble salts present on the surface, raising the electrical conductivity of the water. The measured increase in conductivity establishes the concentration of soluble salts.

plus-icon
minus-icon

Do your instruments require any formal training for use? Do you offer ‘demo’ models?

No. Our surface conducitivity probes are designed for simple operation, feature easy-to-use menus, instruction manuals, and helpful videos. In lieu of demonstration models, unlimited technical support is provided via telephone and/or email, and a limited 30-day money back guarantee.

plus-icon
minus-icon

Still need help?

Before returning your gage or instrument for service, review the troubleshooting steps on the Troubleshooting guide, or speak with a member of our technical support team by calling +1-315-393-4450.

Accessories

PosiPatchPosiPatch

Reusable Bresle Test patch with Standard or Flexible magnetic ring for soluble salt testing

Learn MoreLearn More
Latex Adhesive PatchLatex Adhesive Patch

Latex Bresle Test patch with easy-open tabs and low-tack adhesive for easy removal for soluble salt testing

Learn MoreLearn More
DeFelsko Adhesive PatchDeFelsko Adhesive Patch

Self-adhesive, polyurethane Bresle Test patches for soluble salt testing

Learn MoreLearn More
PosiTector Gage BodiesPosiTector Gage Bodies

PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.

Learn MoreLearn More
PosiTector ProbesPosiTector Probes

PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.

Learn MoreLearn More
Bluetooth PrinterBluetooth Printer

Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.

Learn MoreLearn More
PosiPatch Starter KitPosiPatch Starter Kit

For use with existing conductivity meters. Try the revolutionary, reusable Bresle Method PosiPatch with a low cost trial pack.

Learn MoreLearn More
Standard or Flexible Magnetic RingStandard or Flexible Magnetic Ring

For use with the innovative PosiPatch. Holds Bresle test patches on steel surfaces without leaving any messy residue.

Learn MoreLearn More
PosiTector SST Abrasives Test KitPosiTector SST Abrasives Test Kit

Measures the concentration of water-soluble contaminates in blast cleaning abrasives

Learn MoreLearn More
AC Power KitAC Power Kit

Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.

Learn MoreLearn More
Deionized WaterDeionized Water

Purified, ion-free water to be used with the PosiTector SST, 250 ml or 1 l

Learn MoreLearn More
Pelican Cases for PosiTector Inspection KitsPelican Cases for PosiTector Inspection Kits

Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTector instrument.

Learn MoreLearn More
Certified Conductivity StandardCertified Conductivity Standard

To verify accuracy of PosiTector SST probe

Learn MoreLearn More
Dispensing TipsDispensing Tips

Plastic dispensing tips for the PosiTector SST (10 pack)

Learn MoreLearn More
Belt ClipBelt Clip

Belt Clip for PosiTector gage bodies

Learn MoreLearn More
Protective Lens ShieldProtective Lens Shield

Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.