uparrow-iconp0chonk

PosiTector® 6000

Coating Thickness Gages for ALL Metal Substrates

The rugged, fully electronic PosiTector 6000 Paint Thickness Gage uses magnetic and eddy current principles to measure paint thickness on both ferrous and non-ferrous metals, accurately and quickly.

  • Ready to measure—no calibration adjustment required for most applications
  • Large 2.8" impact resistant color touchscreen with redesigned keypad for quick menu navigation
  • Weatherproof, dustproof, and water-resistant—IP65-rated enclosure
  • Durable wear face and ruby-tip probe for long-lasting calibration
  • PosiTector interchangeable platform—attach any PosiTector probe to a single gage body
  • USB, WiFi, and Bluetooth connectivity to PosiSoft PC, Mac, and Smartphone software
  • Certificate of Calibration showing traceability to NIST or PTB included (Long Form)
Conforms to ISO 2178/2360/2808, ISO 19840, ASTM B244/B499/D1186/D1400/D7091/E376/G12, BS3900-C5, SSPC-PA2, US Navy NAVSEA PPI 63101-000, US Navy NAVSEA 009-32, AS 2331.1.4, AS3894.3-B, and others

Features

simple icon

Simple

  • Fast measurement speed—60+ readings per minute. Enhanced FAST mode—90+ readings per minute for quick inspection.
  • Ready to measure—no adjustment required for most applications
  • Large 2.8" impact resistant color touchscreen with redesigned keypad for quick menu navigation
  • On-gage help explains menu items at the touch of a button
  • Flashing display—ideal in a noisy environment
  • RESET feature instantly restores factory settings
durable icon

Durable

  • Weatherproof, dustproof, and water-resistant—IP65-rated enclosure
  • Ergonomic design with durable rubberized grip
  • NEW Zirconia-toughened wear face and durable ruby-tip for long life, continuous accuracy, and unmatched durability (FS, FTS, FNS, FNDS, FNTS, FRS, FNRS probes only)
  • Shock-absorbing, protective rubber holster for added impact resistance
  • Two year warranty on gage body AND probe
accurate icon

Accurate

  • Certificate of Calibration showing traceability to NIST or PTB included
  • Built-in temperature compensation ensures measurement accuracy
  • Hi-RES mode increases displayed resolution for precision applications
  • Conforms to national and international standards including ISO and ASTM
versatile icon

Versatile

  • PosiTector body accepts all PosiTector 6000, 200, RTR, SPG, DPM, IRT, SST, UTG, SHD, BHI, and GLS probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, ultrasonic wall thickness gage, hardness tester, or gloss meter
  • Multiple Calibration adjustment options including 1 point, 2 point, and ISO 19840 correction factors
  • Selectable display languages
  • Auto rotating display with Flip Lock
  • Extended cables available (up to 75 m/250 ft) for underwater or remote measuring
  • Mils/Microns/mm switchable

Powerful

  • Statistics mode continually displays/updates average, standard deviation, min/max and number of readings while measuring
  • Screen Capture—save 100 screen images for record keeping and review
  • HiLo alarm audibly and visibly alerts when measurements exceed user-specified limits
  • Instant-on feature quickly powers up the gage if recently powered down
  • Over 20 hours of continuous operation with 3 AAA batteries
  • USB port for fast, simple connection to a PC and to supply continuous power. USB cable included.
  • Every stored measurement is date and time stamped
  • Software Updates via web keep your gage current
  • Software Solutions for viewing, analyzing & reporting data

Standard Models

Includes ALL features as shown on left plus...
Includes ALL features as shown above plus...
  • NEW Storage of 1,000 readings per probe—stored readings can be viewed or downloaded

Advanced Models

Includes ALL features as shown on left plus...
Includes ALL features as shown above plus...
  • Storage of 250,000 readings in up to 1,000 batches and sub-batches
  • Live graphing of measurement data
  • Prompted Batch Mode—create pre-defined batches with on-screen text and image prompts for each reading
  • 3 Scan Modes — increase measurement speed to 180+ readings per minute
  • Normal – take continuous readings without lifting the probe
  • Statistics – take continuous readings and record average, standard deviation, min/max thickness and number of readings while scanning
  • Limited Count Average – take continuous readings up to a user-specified count. The gage displays and records the average of the readings.
  • Touchscreen keyboard for quickly renaming batches, adding notes, and more
  • Multiple stored calibration adjustments for measuring on a variety of substrate conditions
  • Calibration Adjustment Reporting feature documents calibration adjustments into PosiSoft software reports
  • SSPC-PA 2, ISO 19840, and IMO PSPC 90/10 modes help users comply with standards by prompting for min/max specifications, displaying the necessary readings, and automatically calculating statistics with a pass/fail result
  • WiFi technology wirelessly synchronizes with PosiSoft.net and downloads software updates
  • Bluetooth 4.0 Technology for data transfer to a mobile device running the PosiTector App or optional portable printer. BLE API available for integration into third-party software
  • Integrate with third-party software, drones, ROVs, PLCs, and robotic devices using several industry-standard communication protocols
  • Connect a Bluetooth barcode scanner or keyboard to instantly annotate readings and batches
View More Features

Models

externallink-icon
View PDF Order Guide

Step 1: Choose a gage body

Step 2: Choose material type

Step 3: Select a model

Click model to download cutsheet
Our most popular Integral and Regular cabled probe models
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Measuring Range:
0 - 80 mils       0 - 2000 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
*FXS Xtreme probe with Alumina wear face and braided cable. Ideal for rough or hot surfaces up to 250 ̊ C (500 ̊ F).
Ideal for Duplex Coating Systems
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Microprobes – Our smallest probes for small parts or hard-to-reach areas
Measuring Range:
0 - 45 mils        0 - 1150 μm
Accuracy
± (0.02 mils + 1%) 0-4 mils
± (0.1 mils + 3%) >4 mils
± (0.5 μm + 1%) 0-100 μm  
± (2 μm + 3%) >100 μm
Integral and Cabled probes for thick protective coatings; epoxy, rubber, intumescent fireproofing and more
Measuring Range:
0 - 250 mils       0 - 6 mm
Accuracy
± (0.5 mils + 1%) 0-100 mils
± (0.5 mils + 3%) >100 mils
± (0.01 mm + 1%) 0-2.5 mm 
± (0.01 mm + 3%) >2.5 mm
Measuring Range:
0 - 400 mils     0 - 10,000 μm
Accuracy
± (0.1 mils + 3%)
± (2 μm + 3%)
**FHXS Xtreme probe with Alumina wear face and braided cable measures non-conductive coatings on steel. Ideal for rough or hot surfaces up to 250 ̊ C (500 ̊ F).
Measuring Range:
0 - 500 mils       0 - 13 mm
Accuracy
± (1 mil + 3%)
± (0.02 mm + 3%)
Measuring Range:
0 - 1.0 in.      0 - 25 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
Measuring Range:
0 - 1.5 inches       0 - 38 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
Measuring Range:
0–2.5 inches       0–63.5 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
*FNGS probe measures non-conductive coatings on all metals.

Step 3: Select a model

Click model to download cutsheet
Our most popular Integral and Regular cabled probe models
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Ideal for anodized aluminum
Measuring Range:
0 - 25 mils       0 - 625 μm
Accuracy
± (0.02 mils + 1%) 0-4 mils
± (0.1 mils + 3%) >4 mils
± (0.5 μm + 1%) 0-100 μm  
± (2 μm + 3%) >100 μm
Microprobes – Our smallest probes for small parts or hard-to-reach areas
Measuring Range:
0 - 25 mils       0 - 625 μm
Accuracy
± (0.02 mils + 1%) 0-4 mils
± (0.1 mils + 3%) >4 mils
± (0.5 μm + 1%) 0-100 μm  
± (2 μm + 3%) >100 μm
Integral and Cabled probes for thick protective coatings; epoxy, rubber, intumescent fireproofing and more
Measuring Range:
0 - 500 mils       0 - 13 mm
Accuracy
± (1 mil + 3%)
± (0.02 mm + 3%)
Measuring Range:
0–2.5 inches       0–63.5 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
*FNGS probe measures non-conductive coatings on all metals.

Step 3: Select a model

Click model to download cutsheet
Our most popular Integral and Regular cabled probe models
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Ideal for Duplex Coating Systems
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Integral and Cabled probes for thick protective coatings; epoxy, rubber, intumescent fireproofing and more
Measuring Range:
0–250 mils       0–6 mm
Accuracy
± (0.5 mils + 1%) 0-100 mils
± (0.5 mils + 3%) >100 mils
± (0.01 mm + 1%) 0-2.5 mm
± (0.01 mm + 3%) >2.5 mm
Measuring Range:
0–2.5 inches       0–63.5 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
*FNGS probe measures non-conductive coatings on all metals.

Step 2: Choose material type

Step 3: Select a model

Click model to download cutsheet
Our most popular Integral and Regular cabled probe models
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Measuring Range:
0 - 80 mils       0 - 2000 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
*FXS Xtreme probe with Alumina wear face and braided cable. Ideal for rough or hot surfaces up to 250 ̊ C (500 ̊ F).
Ideal for Duplex Coating Systems
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Microprobes – Our smallest probes for small parts or hard-to-reach areas
Measuring Range:
0 - 45 mils        0 - 1150 μm
Accuracy
± (0.02 mils + 1%) 0-4 mils
± (0.1 mils + 3%) >4 mils
± (0.5 μm + 1%) 0-100 μm  
± (2 μm + 3%) >100 μm
Integral and Cabled probes for thick protective coatings; epoxy, rubber, intumescent fireproofing and more
Measuring Range:
0 - 250 mils       0 - 6 mm
Accuracy
± (0.5 mils + 1%) 0-100 mils
± (0.5 mils + 3%) >100 mils
± (0.01 mm + 1%) 0-2.5 mm 
± (0.01 mm + 3%) >2.5 mm
Measuring Range:
0 - 400 mils     0 - 10,000 μm
Accuracy
± (0.1 mils + 3%)
± (2 μm + 3%)
**FHXS Xtreme probe with Alumina wear face and braided cable measures non-conductive coatings on steel. Ideal for rough or hot surfaces up to 250 ̊ C (500 ̊ F).
Measuring Range:
0 - 500 mils       0 - 13 mm
Accuracy
± (1 mil + 3%)
± (0.02 mm + 3%)
Measuring Range:
0 - 1.0 in.      0 - 25 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
Measuring Range:
0 - 1.5 inches       0 - 38 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
Measuring Range:
0–2.5 inches       0–63.5 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
*FNGS probe measures non-conductive coatings on all metals.

Step 3: Select a model

Click model to download cutsheet
Our most popular Integral and Regular cabled probe models
Measuring Range:
0 - 60 mils    0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Ideal for anodized aluminum
Measuring Range:
0 - 25 mils       0 - 625 μm
Accuracy
± (0.02 mils + 1%) 0-4 mils
± (0.1 mils + 3%) >4 mils
± (0.5 μm + 1%) 0-100 μm  
± (2 μm + 3%) >100 μm
Microprobes – Our smallest probes for small parts or hard-to-reach areas
Measuring Range:
0 - 25 mils       0 - 625 μm
Accuracy
± (0.02 mils + 1%) 0-4 mils
± (0.1 mils + 3%) >4 mils
± (0.5 μm + 1%) 0-100 μm  
± (2 μm + 3%) >100 μm
Integral and Cabled probes for thick protective coatings; epoxy, rubber, intumescent fireproofing and more
Measuring Range:
0 - 500 mils       0 - 13 mm
Accuracy
± (1 mil + 3%)
± (0.02 mm + 3%)
Measuring Range:
0–2.5 inches       0–63.5 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
*FNGS probe measures non-conductive coatings on all metals.

Step 3: Select a model

Click model to download cutsheet
Our most popular Integral and Regular cabled probe models
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Ideal for Duplex Coating Systems
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils + 1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Integral and Cabled probes for thick protective coatings; epoxy, rubber, intumescent fireproofing and more
Measuring Range:
0 - 250 mils       0 - 6 mm
Accuracy
± (0.5 mils + 1%) 0-100 mils
± (0.5 mils + 3%) >100 mils
± (0.01 mm + 1%) 0-2.5 mm
± (0.01 mm + 3%) >2.5 mm
Measuring Range:
0 - 2.5 inches       0 - 63.5 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
*FNGS probe measures non-conductive coatings on all metals.
SmartLink and app in use

PosiTector SmartLink - A Smart New Way to Measure

PosiTector SmartLink and free mobile app turns your cell phone or tablet into a virtual PosiTector gage.

Wirelessly connect PosiTector probes to your Apple iOS or Android smart device.

For more information about the PosiTector SmartLink, click here.

Step 2: Choose material type

Step 3: Select a model

Click model to download cutsheet
Our most popular Integral and Regular cabled probe models
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Measuring Range:
0 - 80 mils       0 - 2000 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
*FXS Xtreme probe with Alumina wear face and braided cable. Ideal for rough or hot surfaces up to 250 ̊ C (500 ̊ F).
Ideal for Duplex Coating Systems
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Microprobes – Our smallest probes for small parts or hard-to-reach areas
Measuring Range:
0 - 45 mils       0 - 1150 μm
Accuracy
± (0.02 mils + 1%) 0-4 mils
± (0.1 mils + 3%) >4 mils
± (0.5 μm + 1%) 0-100 μm  
± (2 μm + 3%) >100 μm
Integral and Cabled probes for thick protective coatings; epoxy, rubber, intumescent fireproofing and more
Measuring Range:
0 - 250 mils       0 - 6 mm
Accuracy
± (0.5 mils + 1%) 0-100 mils
± (0.5 mils + 3%) >100 mils
± (0.01 mm + 1%) 0-2.5 mm 
± (0.01 mm + 3%) >2.5 mm
Measuring Range:
0 - 400 mils     0 - 10,000 μm
Accuracy
± (0.1 mils + 3%)
± (2 μm + 3%)
**FHXS Xtreme probe with Alumina wear face and braided cable measures non-conductive coatings on steel. Ideal for rough or hot surfaces up to 250 ̊ C (500 ̊ F).
Measuring Range:
0 - 500 mils       0 - 13 mm
Accuracy
± (1 mil + 3%)
± (0.02 mm + 3%)
Measuring Range:
0 - 1.0 in.      0 - 25 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
Measuring Range:
0 - 1.5 inches       0 - 38 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
Measuring Range:
0 - 2.5 inches       0 - 63.5 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
*FNGS probe measures non-conductive coatings on all metals.

Step 3: Select a model

Click model to download cutsheet
Our most popular Integral and Regular cabled probe models
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
Ideal for anodizing aluminum
Measuring Range:
0 - 25mils       0 - 625μm
Accuracy
± (0.02 mils + 1%) 0-4 mils
± (0.1 mils + 3%) >4 mils
± (0.5 μm + 1%) 0-100 μm  
± (2 μm + 3%) >100 μm
Microprobes – Our smallest probes for small parts or hard-to-reach areas
Measuring Range:
0 - 25 mils       0 - 625 μm
Accuracy
± (0.02 mils + 1%) 0-4 mils
± (0.1 mils + 3%) >4 mils
± (0.5 μm + 1%) 0-100 μm  
± (2 μm + 3%) >100 μm
Integral and Cabled probes for thick protective coatings; epoxy, rubber, intumescent fireproofing and more
Measuring Range:
0 - 500 mils       0 - 13 mm
Accuracy
± (1 mil + 3%)
± (0.02 mm + 3%)
Measuring Range:
0 - 2.5 inches       0 - 63.5 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
*FNGS probe measures non-conductive coatings on all metals.

Step 3: Select a model

Click model to download cutsheet
Our most popular Integral and Regular cabled probe models
Measuring Range:
0 - 60 mils       0 - 1500 μm
Accuracy
± (0.05 mils + 1%) 0 - 2 mils  
± (0.1 mils  +  1%) > 2 mils
± (1 μm + 1%)  0 - 50 μm  
± (2 μm + 1%)  > 50 μm
*Ideal for duplex coating systems
Integral and Cabled probes for thick protective coatings; epoxy, rubber, intumescent fireproofing and more
Measuring Range:
0 - 250 mils       0 - 6 mm
Accuracy
± (0.5 mils + 1%) 0 - 100 mils
± (0.5 mils + 3%) > 100 mils
± (0.01 mm + 1%) 0 - 2.5 mm
± (0.01 mm + 3%) > 2.5 mm
Measuring Range:
0 - 2.5 inches       0 - 63.5 mm
Accuracy
± (0.01 in. + 3%)
± (0.2 mm + 3%)
*FNGS probe measures non-conductive coatings on all metals.

Videos

Video Thumbnail
DeFelsko Coating Thickness Gages | 2023
Video Thumbnail
How to Use IMO PSPC 90/10 Mode for Measuring Coating Thickness with the PosiTector 6000
Video Thumbnail
How to Use ISO 19840 Mode for Measuring Coating Thickness with the PosiTector 6000
Video Thumbnail
Saving Money and Time with PosiTector Probe Interchangeability
Video Thumbnail
How to Use SSPC-PA2 Mode for Measuring Coating Thickness with the PosiTector 6000
Video Thumbnail
How To Use Prompted Batch Mode to Simplify Inspections and Maximize Performance
Video Thumbnail
How to Measure Coating and Paint Thickness with the PosiTector 6000
Video Thumbnail
New PosiTector Gage Body
Video Thumbnail
PosiTector SmartLink

FNTS

Ferrous & Non-Ferrous
0 - 250 mils (0 - 6 mm)
Add to Instant Quote

FNS

Ferrous & Non-Ferrous
0 - 60 mils (0 - 1500 µm)
Add to Instant Quote

FN

Ferrous & Non-Ferrous
0 - 60 mils (0 - 1500 µm)
Add to Instant Quote

N90S

Non-Ferrous
0 - 25 mils (0 - 625 µm)
Add to Instant Quote

N45S

Non-Ferrous
0 - 25 mils (0 - 625 µm)
Add to Instant Quote

NAS

Non-Ferrous
0 - 25 mils (0 - 625 µm)
Add to Instant Quote

NRS

Non-Ferrous
0 - 60 mils (0 - 1500 µm)
Add to Instant Quote

NS

Non-Ferrous
0 - 60 mils (0 - 1500 µm)
Add to Instant Quote

FNGS

Ferrous & Non-Ferrous
0 - 2.5 inches (0 - 63.5 mm)
Add to Instant Quote

FLS

Ferrous
0 - 1.5 inches (0 - 38 mm)
Add to Instant Quote

FJS

Ferrous
0 - 1.0 inch (0 - 25 mm)
Add to Instant Quote

FKS

Ferrous
0 - 500 mils (0 - 13 mm)
Add to Instant Quote

FTRS

Ferrous
0 - 250 mils (0 - 6 mm)
Add to Instant Quote

FTS

Ferrous
0 - 250 mils (0 - 6 mm)
Add to Instant Quote

FT

Ferrous
0 - 250 mils (0 - 6 mm)
Add to Instant Quote

F90ES

Ferrous
0 - 45 mils (0 - 1150 µm)
Add to Instant Quote

F90S

Ferrous
0 - 45 mils (0 - 1150 µm)
Add to Instant Quote

F0S

Ferrous
0 - 45 mils (0 - 1150 µm)
Add to Instant Quote

FNDS

Ferrous & Non-Ferrous
0 - 60 mils (0 - 1500 µm)
Add to Instant Quote

N0S

Non-Ferrous
0 - 25 mils (0 - 625 µm)
Add to Instant Quote

F45S

Ferrous
0 - 45 mils (0 - 1150 µm)
Add to Instant Quote

FHXS

Ferrous
0 - 400 mils (0 - 10 mm)
Add to Instant Quote

FXS

Ferrous
0 - 80 mils (0 - 2000 µm)
Add to Instant Quote

NKS

Non-Ferrous
0 - 500 mils (0 - 13 mm)
Add to Instant Quote

FNRS

Ferrous & Non-Ferrous
0 - 60 mils (0 - 1500 µm)
Add to Instant Quote

N

Non-Ferrous
0 - 60 mils (0 - 1500 µm)
Add to Instant Quote

FRS

Ferrous
0 - 60 mils (0 - 1500 µm)
Add to Instant Quote

FS

Ferrous
0 - 60 mils (0 - 1500 µm)
Add to Instant Quote

F

Ferrous
0 - 60 mils (0 - 1500 µm)
Add to Instant Quote

Software

PosiSoft Software in use

PosiSoft Desktop

Powerful desktop software for downloading, archiving, and reporting measurement data. No internet connection required.

  • Simple, intuitive user interface
  • Import readings directly from the gage via USB, WiFi, or legacy PosiSoft Desktop versions
  • Fully integrates with PosiSoft.net—backup and synchronize jobs, batches, readings, and report templates to the cloud. Click here to learn more about PosiSoft.net
Learn More

PosiTector App

An easy-to-use mobile app (iOS/ Android) that connects to your PosiTector Advanced, PosiTector Smartlink, or PosiTest AT-A. Compatible with PosiSoft.net.

Learn More

PosiSoft USB

A simple gage interface to retrieve data in a manner similar to a flash drive. No software to install or internet connection required.

Learn More

PosiSoft Custom PDF Report Generator

featured on PosiSoft Desktop, PosiSoft.net, PosiTector App
Easily create reports from your measurement data in seconds
  • Generate custom, professional PDF reports
  • Include inspection information such as on-site pictures, screen captures, notes and more to communicate important details
  • Create and save multiple custom layouts as templates – insert cover pages, add logos/images, and select font and point size
  • Select the information to include for each product type – charts, histograms, readings, time stamps and more
  • Compile multi-batch reports from one or more probes and instrument types

PosiSoft.net

PosiSoft.net is a free cloud-based application offering secure storage of PosiTector and PosiTest Inspection Instrument data. Click Here to learn more.

PosiTector Developer Resources

From wired USB to WiFi wireless technology, DeFelsko instruments offer data management solutions for even the most advanced software integrations. Accessing your stored or live streaming data is simpler and more flexible than ever before. PosiTector and PosiTest AT-A instruments have the ability to integrate with third-party software, drones, ROVs, PLCs, and robotic devices using several industry-standard communication protocols.

Learn More about Integrating Third-Party Devices and Applications

F.A.Q.

plus-icon
minus-icon

Is the PosiTector 6000 calibrated at the factory?

PosiTector 6000 paint meters arrive fully calibrated and include a Long-Form Certificate of Calibration traceable to NIST or PTB. The Certificate of Calibration documents actual readings taken by your instrument at our calibration laboratory, on standards traceable to a national metrology institute. Beware of ‘Certificates’ or ‘Certificates of Conformance’ offered by competitors. These typically do not include actual instrument readings, and are often insufficient to meet common quality requirements.

plus-icon
minus-icon

Does the PosiTector 6000 need to be ‘calibrated’ or ‘adjusted’ prior to use? Do I need to perform a two-point adjustment prior to measuring?

The innovative probe technology and factory calibration in the PosiTector 6000 means that it arrives ready-to-measure — usually there is no need to perform a two-point calibration adjustment. Zirconia-toughened, alumina, or ruby probe tip models eliminate wear, meaning that the factory calibration is maintained throughout the lifetime of the probe. Whether out of the box or after years of use, the PosiTector 6000 Paint Thickness Gauge will continue to provide accurate results.

For highest confidence and best measurement accuracy, observe our “golden rule” — simply check ZERO (or the known thickness of a shim) on the uncoated part, adjust if necessary, and then measure the coated part. This ensures that the probe is properly adjusted for substrate characteristics including mass, metallurgy, curvature, temperature and roughness.

plus-icon
minus-icon

Do your instruments require any formal training for use? Do you offer ‘demo’ models?

No. Our instruments are designed for simple operation, feature easy-to-use menus, instruction manuals, and helpful videos. In lieu of demonstration models, we provide unlimited technical support via telephone and/or email, and a limited 30-day money back guarantee.

plus-icon
minus-icon

How often should the PosiTector 6000 be recalibrated?

PosiTector 6000 paint thickness probes include a Certificate of Calibration with no expiry or end date. They have no shelf life, therefore the length of time in the field is not a good indicator for recalibration intervals. Many organizations with quality programs and recertification programs require annual recalibrations, and this is a good starting point for most users. DeFelsko recommends that customers establish calibration intervals based upon their own experience and work environment. Based on our product knowledge, data and customer feedback, a one year calibration interval from the date the instrument was placed in service is a good starting point.

plus-icon
minus-icon

What can the PosiTector 6000 measure?

PosiTector 6000 paint thickness probes have different capabilities depending on the model.

  • ‘Ferrous’ model probes (order code beginning in ‘F’
    ex. FS1) can measure non-magnetic coatings applied to ferrous (magnetic) metals, typically carbon steel.
  • ‘Non-ferrous’ model probes (order code beginning in ‘N’ ex. NRS3) can measure non-conductive coatings applied to non-ferrous metals.
  • ‘Combination model probes (order code beginning in ‘FN’ ex. FNTS1) can measure non-magnetic coatings applied to ferrous (magnetic) metals, AND non-conductive coatings applied to non-ferrous metals
plus-icon
minus-icon

Is the PosiTector 6000 affected by the surface roughness (profile) of the metal substrate below the coating?

All coating thickness gages are influenced to some degree by substrate roughness, as shown in the below image. It is generally accepted that paint thickness should be measured from the highest ‘peaks’ in the rough surface thus ensuring they are covered by the protective coating. However, coating thickness gages will instead measure the coating thickness from the ‘effective magnetic plane’, which is located somewhere between the highest peaks and deepest valleys of the profile.

ASTM D7091, ISO 19840, and SSPC-PA 2 propose several similar solutions depending upon the instrument type and the particular situation. One option is to verify the paint meter reads zero on the uncoated steel substrate, and adjust to zero if necessary. This is a popular solution when the metal surface is smooth.

Since it is difficult to ensure that the probe tip is sitting on the highest peaks of the surface profile, the preferred option is to place a plastic shim of a known thickness that is close to the expected thickness of the applied coating between the probe and substrate and adjust to the stated thickness of the shim- referred to as a 1-point adjustment. The plastic shim sits on the peaks of the surface profile over a greater area than the probe tip, ensuring that the adjustment is being taken ‘over the peaks’. This best simulates a coating covering the peaks of the surface profile.

If access to the bare substrate is not possible, another option is to use the PosiTector Zero Offset feature in accordance with ISO 19840. The Zero Offset adjustment is useful when measuring paint and coating thickness over rough or blasted substrates without access to the uncoated representative substrate. Predefined Zero Offset values can be selected according to the blast profile height. Alternatively, a custom Zero Offset can be entered.

plus-icon
minus-icon

Can the PosiTector 6000 measure coatings on stainless steel?

"Stainless steel" is a term used to generally categorize a wide variety of corrosion and heat-resistant alloys. In specific terms of metallurgy, a “stainless steel” is any iron-based alloy containing a minimum of 10.5% chromium content by mass. Some stainless steel alloys have a relatively low magnetic response (often called “partially/weakly magnetic”). Others have no magnetic response whatsoever, and some possess a ferromagnetic response similar to carbon steel.

The PosiTector 6000 Coating Thickness Gauge is uniquely able to measure partially magnetic stainless steel alloys, an application that is challenging for many competitive instruments. PosiTector 6000 FN (combination ferrous/non-ferrous) probe models can often measure consistently on partially magnetic substrates with a simple Zero adjustment. For more challenging applications, the “N-Lock” measurement mode permits accurate measurement of non-conductive coatings applied to partially magnetic substrates.

For more information, read How to Measure Coatings on Stainless Steel.

plus-icon
minus-icon

Can the PosiTector 6000 measure coatings on hot surfaces?

The PosiTector 6000 FXS and FHXS Xtreme probes are ideal for measuring coating thickness on hot and/or rough surfaces (250°C, 500°F maximum). All PosiTector 6000 coating thickness probes are capable of measuring on hot surfaces. Standard probe models can operate at environments up to 50˚C (120˚F). However, if the probe is lifted clear of the surface as soon as a reading is taken and is allowed to cool, thickness measurements can be taken at higher temperatures. Simply ensure that the probe remains at a temperature of less than 50˚C (120˚F), and cool enough to handle with an unprotected hand.

plus-icon
minus-icon

What is the minimum part size required to take a reading?

To ensure a part’s dimensions are suitable for a PosiTector 6000 probe, simply check ZERO on the uncoated part and adjust if necessary. Verify accuracy by measuring a plastic shim placed on the uncoated part. If the measurement is within the combined tolerances of the shim and probe, the probe is suitable for measuring the coated part.

plus-icon
minus-icon

Can the PosiTector 6000 be used underwater?

While the PosiTector gage body and probe connector are not suitable for immersion in water, PosiTector 6000 regular cabled probes are hermetically sealed and ideal for underwater use. Extended cables are available (up to 75 m/250 ft) for underwater or remote measuring.

plus-icon
minus-icon

Is the PosiTector 6000 intrinsically safe?

While the PosiTector 6000 Coating Thickness Tester is not designed as an intrinsically safe device, our PosiTest mechanical gages are ideal for measuring coating thickness in hazardous operating environments.

plus-icon
minus-icon

Can the PosiTector 6000 measure nickel on steel?

Yes, but it depends upon the particular type of nickel coating that has been applied to the steel.

  • When nickel plating is deposited by a process of electrolysis (employing an electric current in the nickel bath), the resultant coating – commonly called “e-nickel” – is always conductive and magnetic to some degree and cannot be accurately measured by our mil gages when applied to ferrous or non-ferrous metals.
  • Electroless nickel coatings are deposited by an autocatalytic process which does not involve the addition of an electric current. If the nickel bath in this process contains a minimum concentration of ~8% phosphorus, the resulting nickel plating is effectively non-magnetic and its thickness can be accurately measured on ferrous steel with a magnetic principle coating thickness gage such as a PosiTector 6000 F model.
plus-icon
minus-icon

What is the measurement range of the PosiTector 6000?

The coating thickness measurement range of the PosiTector 6000 paint meter is dependent on which interchangeable probe is attached. PosiTector 6000 probes are available for measuring a wide variety of coating thickness applications.  For example, the PosiTector 6000 FN probe can measure coating thicknesses up to 1500 um (60 mils), while the PosiTector 6000 FNGS probe measures coatings up to 63.5 mm (2.5 inches) thick. No matter your application, DeFelsko likely has a measuring solution to satisfy your requirement.

plus-icon
minus-icon

What is a mil?

A mil, also known as a Thou, is equal to 1 one-thousandth of an inch (25.4 microns).

plus-icon
minus-icon

What is a micron?

A micron, sometimes called a micrometer, is equal to one-millionth of a meter or one-thousandth of a millimeter (~0.000039").

plus-icon
minus-icon

Still need help?

Before returning your gage or instrument for service, review the troubleshooting steps on the Troubleshooting guide, or speak with a member of our technical support team by calling +1-315-393-4450.

Accessories

PosiTector Gage BodiesPosiTector Gage Bodies

PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.

Learn MoreLearn More
PosiTector ProbesPosiTector Probes

PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.

Learn MoreLearn More
Bluetooth PrinterBluetooth Printer

Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.

Learn MoreLearn More
Certified Thickness StandardsCertified Thickness Standards

Verify accuracy/operation of coating thickness gages. Important component of fulfilling both ISO/QS-9000 and in-house quality control requirements with a measurement accuracy traceable to NIST or PTB.

Learn MoreLearn More
PosiTector CasePosiTector Case

Convenient hard shell case for carrying a PosiTector gage body and multiple probes

Learn MoreLearn More
Certified Plastic ShimsCertified Plastic Shims

Economical alternative to Coated Metal Plates, with a reduced accuracy. Ideal for protecting the PosiTector probe tip.

Learn MoreLearn More
Telescopic Probe ExtenderTelescopic Probe Extender

A lightweight, portable device that allows you to extend the reach of your PosiTector 6000 regular cabled probes.

Learn MoreLearn More
AC Power KitAC Power Kit

Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.

Learn MoreLearn More
Pelican Cases for PosiTector Inspection KitsPelican Cases for PosiTector Inspection Kits

Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTector instrument.

Learn MoreLearn More
Belt ClipBelt Clip

Belt Clip for PosiTector gage bodies

Learn MoreLearn More
Certified Polystyrene BlocksCertified Polystyrene Blocks

Certified Polystyrene Blocks are for use with gages that measure over 1500 µm (60 mils).

Learn MoreLearn More
Probe Foot RingsProbe Foot Rings

Ideal for use on thin, soft coatings to protect coatings from unnecessary wear while using Scan or Fast mode to measure large objects

Learn MoreLearn More
Probe Fixture StandProbe Fixture Stand

Helps reduce adverse operator influence by ensuring the PosiTector 6000 probe is placed perpendicular to the part’s surface in a controlled, repeatable way.

Learn MoreLearn More
Non-Certified Plastic ShimsNon-Certified Plastic Shims

Provide a quick operational check of the instrument by allowing the user to perform practice measurements

Learn MoreLearn More
Protective Lens ShieldProtective Lens Shield

Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.

Learn MoreLearn More
View More Accessories